GEOPOLYMER MORTAR AND METHOD
A geopolymer mortar formed by mixing about 35% to about 45% by weight pozzolanic material, about 35% to about 45% by weight silicon oxide source, about 15% to about 20% by weight alkaline activator solution, and about 0.3% to about 2.5% by weight copper ion source. The pozzolanic material may be fly ash and the silicon oxide source may be sand. The alkaline activator solution may be a sodium hydroxide solution containing sodium silicate. The geopolymer mortar may have a viscosity in the range of about 25,000 to about 50,000 centipoise. The geopolymer mortar may be formed by further mixing one or more additives, such as surfactants, thermal spheres, anti-sagging agents, adhesion primers, or fibers. The geopolymer mortar may be applied as a protective coating on a surface of a structure.
GEOPOLYMER MORTAR AND METHOD
A geopolymer mortar formed by mixing about 35% to about 45% by weight pozzolanic material, about 35% to about 45% by weight silicon oxide source, about 15% to about 20% by weight alkaline activator solution, and about 0.3% to about 2.5% by weight copper ion source. The pozzolanic material may be fly ash and the silicon oxide source may be sand. The alkaline activator solution may be a sodium hydroxide solution containing sodium silicate. The geopolymer mortar may have a viscosity in the range of about 25,000 to about 50,000 centipoise. The geopolymer mortar may be formed by further mixing one or more additives, such as surfactants, thermal spheres, anti-sagging agents, adhesion primers, or fibers. The geopolymer mortar may be applied as a protective coating on a surface of a structure.
GEOPOLYMER MORTAR AND METHOD
MORTIER DE GEOPOLYMERE ET PROCEDE
ALLOUCHE EREZ (author) / MONTES CARLOS (author)
2016-04-05
Patent
Electronic Resource
English