The invention discloses a ceramic bond and a preparation method thereof. The ceramic bond is prepared from the following substances in parts by weight: 20-30 parts of Na2O, 30-40 parts of B2O3, 45-50 parts of Al2O3, 15-30 parts of SiO2, 8-10 parts of Li2CO3, 1-5 parts of KNO3 and 5-10 parts of TiO2. The preparation method comprises the following steps: sufficiently mixing all raw materials in a ball mill; adding water, carrying out ball milling for 10-15 hours, and standing for 3-5 hours; pouring the water out, and baking at 90-110 DEG C; and carrying out ball milling, and screening to prepare the ceramic bond. The prepared ceramic bond has the characteristics of low refractoriness and high strength.
The invention discloses a ceramic bond and a preparation method thereof. The ceramic bond is prepared from the following substances in parts by weight: 20-30 parts of Na2O, 30-40 parts of B2O3, 45-50 parts of Al2O3, 15-30 parts of SiO2, 8-10 parts of Li2CO3, 1-5 parts of KNO3 and 5-10 parts of TiO2. The preparation method comprises the following steps: sufficiently mixing all raw materials in a ball mill; adding water, carrying out ball milling for 10-15 hours, and standing for 3-5 hours; pouring the water out, and baking at 90-110 DEG C; and carrying out ball milling, and screening to prepare the ceramic bond. The prepared ceramic bond has the characteristics of low refractoriness and high strength.
Ceramic bond and preparation method thereof
GAO XINGZU (author)
2015-04-08
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Ceramic bond, preparation method thereof and grinding tool
European Patent Office | 2021
|Low-temperature ceramic bond and preparation method thereof
European Patent Office | 2015
|Ceramic composition, ceramic and preparation method thereof
European Patent Office | 2020
|