Method for preparing slag baking-free brick
The invention relates to a method for preparing slag baking-free brick. The process is simple, the utilization rate of solid wastes is high, and the baking-free brick is light in weight, high in strength, high in durability, low in energy consumption and pollution-free. The preparation method comprises the following steps: uniformly mixing and stirring the raw materials such as cement and slag, vibrating and performing extrusion forming to form the green brick in a mold, performing steam curing for 48 hours, standing outdoors at normal temperature for 10-15 days, thereby obtaining the finished product.
Method for preparing slag baking-free brick
The invention relates to a method for preparing slag baking-free brick. The process is simple, the utilization rate of solid wastes is high, and the baking-free brick is light in weight, high in strength, high in durability, low in energy consumption and pollution-free. The preparation method comprises the following steps: uniformly mixing and stirring the raw materials such as cement and slag, vibrating and performing extrusion forming to form the green brick in a mold, performing steam curing for 48 hours, standing outdoors at normal temperature for 10-15 days, thereby obtaining the finished product.
Method for preparing slag baking-free brick
LIANG ZUOHONG (author)
2015-04-29
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2023
|Method for preparing baking-free brick from harmless aluminum ash and baking-free brick
European Patent Office | 2024
|Baking-free brick containing desulfurization slag and steel slag
European Patent Office | 2021
|Method for preparing baking-free brick from waste and brick product
European Patent Office | 2015
|