Method for manufacturing Nixing pottery imitated bronze wares
The invention provides a method for manufacturing Nixing pottery imitated bronze wares. The method comprises the following steps: 1) blank preparation: uniformly mixing 40-60 parts of dong mud, 20-40 parts of xi mud, 1-2 parts of copper oxide and 0.1-0.5 part of cerium oxide; 2) forming a green body; 3) fettling; 4) decorating the green body; 5) drying the green body; and 6) firing: putting the decorated green body in a kiln to fire; and in the process of firing, gradually increasing the temperature, firstly, increasing the temperature to 550-650 DEG C at a temperature rise speed of 80-130 DEG C/hour, then increasing the temperature to 1050-1080 DEG C at a temperature rise speed of 140-180 DEG C/hour, and at the temperature, continuously firing the green body for 0.5-1 hour, then cooling the green body, and taking out the obtained product, so that a Nixing pottery imitated bronze ware is obtained. The Nixing pottery imitated bronze ware prepared according to the invention is natural and of primitive simplicity, and has a metal texture, so that the Nixing pottery imitated bronze ware can show an artistic effect of decorousness and classic elegance and a historical decorous feeling better, therefore, the Nixing pottery imitated bronze ware has a rich collection value.
Method for manufacturing Nixing pottery imitated bronze wares
The invention provides a method for manufacturing Nixing pottery imitated bronze wares. The method comprises the following steps: 1) blank preparation: uniformly mixing 40-60 parts of dong mud, 20-40 parts of xi mud, 1-2 parts of copper oxide and 0.1-0.5 part of cerium oxide; 2) forming a green body; 3) fettling; 4) decorating the green body; 5) drying the green body; and 6) firing: putting the decorated green body in a kiln to fire; and in the process of firing, gradually increasing the temperature, firstly, increasing the temperature to 550-650 DEG C at a temperature rise speed of 80-130 DEG C/hour, then increasing the temperature to 1050-1080 DEG C at a temperature rise speed of 140-180 DEG C/hour, and at the temperature, continuously firing the green body for 0.5-1 hour, then cooling the green body, and taking out the obtained product, so that a Nixing pottery imitated bronze ware is obtained. The Nixing pottery imitated bronze ware prepared according to the invention is natural and of primitive simplicity, and has a metal texture, so that the Nixing pottery imitated bronze ware can show an artistic effect of decorousness and classic elegance and a historical decorous feeling better, therefore, the Nixing pottery imitated bronze ware has a rich collection value.
Method for manufacturing Nixing pottery imitated bronze wares
WANG ZHUO (author) / WANG ZHAORU (author)
2015-05-20
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME