Preparation method of special-shaped boron carbide ceramic sandblast nozzle
The invention discloses a preparation method of a special-shaped boron carbide ceramic sandblast nozzle. The preparation method comprises the following steps: (1) proportioning all the raw materials in percentage by weight as follows: 50-70wt% of boron carbide powder, 20-40wt% of a sintering aid, 1-8wt% of a carbon source, 0.5-6wt% of an adhesive and 0.6-6wt% of a dispersing agent; (2) carrying out a spray drying granulation process on the obtained slurry into granules; (3) putting the granules into a manufactured soft mould sleeve and moulding by using a dry bag type granules method, thus obtaining a sandblast nozzle biscuit; (4) putting the sandblast nozzle biscuit into a debonding furnace, vacuumizing, heating for removing water and organics, then processing in a vacuum sintering furnace to obtain a finished boron carbide ceramic sandblast nozzle product. The method is suitable for volume production and the prepared boron carbide sandblast nozzle has the advantages of high hardness, good toughness, good wear resistance, long service life, low cost, and high performance cost ratio. The method can be used for preparing sandblast nozzle products with complicated hole structures.
Preparation method of special-shaped boron carbide ceramic sandblast nozzle
The invention discloses a preparation method of a special-shaped boron carbide ceramic sandblast nozzle. The preparation method comprises the following steps: (1) proportioning all the raw materials in percentage by weight as follows: 50-70wt% of boron carbide powder, 20-40wt% of a sintering aid, 1-8wt% of a carbon source, 0.5-6wt% of an adhesive and 0.6-6wt% of a dispersing agent; (2) carrying out a spray drying granulation process on the obtained slurry into granules; (3) putting the granules into a manufactured soft mould sleeve and moulding by using a dry bag type granules method, thus obtaining a sandblast nozzle biscuit; (4) putting the sandblast nozzle biscuit into a debonding furnace, vacuumizing, heating for removing water and organics, then processing in a vacuum sintering furnace to obtain a finished boron carbide ceramic sandblast nozzle product. The method is suitable for volume production and the prepared boron carbide sandblast nozzle has the advantages of high hardness, good toughness, good wear resistance, long service life, low cost, and high performance cost ratio. The method can be used for preparing sandblast nozzle products with complicated hole structures.
Preparation method of special-shaped boron carbide ceramic sandblast nozzle
WU GUOPING (author) / JIAO YONGFENG (author) / SUN XUEPING (author) / XIE FANGMIN (author)
2015-05-20
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Spindle-shaped aggregate toughened boron carbide ceramic and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2020
|