A platform for research: civil engineering, architecture and urbanism
Volcanic rock powder steam-pressing brick
The invention discloses a volcanic rock powder steam-pressing brick. The volcanic rock powder steam-pressing brick comprises, by weight, 10-20 parts of cement, 20-25 parts of slag, 13-15 parts of volcanic rock powder, 4-6 parts of titanium dioxide, 1-2 parts of 2-ethylhexyl epoxystearate, 2-4 parts of shell powder, 1-2 parts of ardealite, 0.3-0.5 part of zirconium boride, 0.4-0.8 part of titanium diboride, 4-5 parts of zeolite powder, 0.2-0.4 part of benzoyl peroxide, 1-1.8 parts of gelatin, 0.1-0.2 part of polyacrylic acid, 0.3-0.8 part of glycerinum and the balance of deionized water.
Volcanic rock powder steam-pressing brick
The invention discloses a volcanic rock powder steam-pressing brick. The volcanic rock powder steam-pressing brick comprises, by weight, 10-20 parts of cement, 20-25 parts of slag, 13-15 parts of volcanic rock powder, 4-6 parts of titanium dioxide, 1-2 parts of 2-ethylhexyl epoxystearate, 2-4 parts of shell powder, 1-2 parts of ardealite, 0.3-0.5 part of zirconium boride, 0.4-0.8 part of titanium diboride, 4-5 parts of zeolite powder, 0.2-0.4 part of benzoyl peroxide, 1-1.8 parts of gelatin, 0.1-0.2 part of polyacrylic acid, 0.3-0.8 part of glycerinum and the balance of deionized water.
Volcanic rock powder steam-pressing brick
WANG CHANGFU (author) / MAO DONGCHAO (author) / WANG YUTONG (author) / LIU WEI (author)
2015-08-05
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
High strength steam-pressing brick containing carbon nano-tubes
European Patent Office | 2015
|European Patent Office | 2024
|Archaized brick framework and archaized brick pressing production method