The invention discloses a waterproof additive which is composed of the following components in parts by weight: 5-10 parts of magnesium sulfate, 1-5 parts of calcium chloride, 1-3 parts of acetic acid, 3-8 parts of sodium hydroxide, 15-30 parts of quick lime, 2-5 parts of talcum powder, and 20-30 parts of water. The waterproof additive disclosed by the invention, which is used in the process of producing building materials, can greatly improve the self water resistance of the building materials, reduce the occurrence of water seepage and leakage, prolong the service lives of the building materials, and improve the long-term use effect of the building materials.
The invention discloses a waterproof additive which is composed of the following components in parts by weight: 5-10 parts of magnesium sulfate, 1-5 parts of calcium chloride, 1-3 parts of acetic acid, 3-8 parts of sodium hydroxide, 15-30 parts of quick lime, 2-5 parts of talcum powder, and 20-30 parts of water. The waterproof additive disclosed by the invention, which is used in the process of producing building materials, can greatly improve the self water resistance of the building materials, reduce the occurrence of water seepage and leakage, prolong the service lives of the building materials, and improve the long-term use effect of the building materials.