Ageing cracking resistant ceramic bowl and preparation method thereof
The invention discloses an ageing cracking resistant ceramic bowl and its preparation method. The ceramic bowl is prepared from the following raw materials, by weight, 33-47 parts of meerschaum, 25-35 parts of leucite, 22-33 parts of barite, 18-26 parts of nacrite, 15-25 parts of glass flake, 4-8 parts of tea dust, 3-6 parts of calcium hexaboride, 9-16 parts of konjaku flour, 4-7 parts of soya lecithin, 2-4 parts of disodium ethylene diamine tetraacetate, 3-5 parts of poly-aluminum ferric silicate sulfate, 2-3 parts of CITREM, 4-6 parts of alkali lignin and 8-10 parts of antimicrobial powder. With addition of glass flake, tea dust and calcium hexaboride, chemical corrosion resistance and ageing resistance of ceramic tiles can be enhanced. In addition, with addition of konjaku flour, soya lecithin, poly-aluminum ferric silicate sulfate and the like, adhesive stress among mineral particles can be raised, and ageing cracking of ceramic tiles can be prevented effectively. The prepared ceramic bowl has excellent heat resistance, corrosion resistance and ageing resistance, is not easy to crack or break and has long service life.
Ageing cracking resistant ceramic bowl and preparation method thereof
The invention discloses an ageing cracking resistant ceramic bowl and its preparation method. The ceramic bowl is prepared from the following raw materials, by weight, 33-47 parts of meerschaum, 25-35 parts of leucite, 22-33 parts of barite, 18-26 parts of nacrite, 15-25 parts of glass flake, 4-8 parts of tea dust, 3-6 parts of calcium hexaboride, 9-16 parts of konjaku flour, 4-7 parts of soya lecithin, 2-4 parts of disodium ethylene diamine tetraacetate, 3-5 parts of poly-aluminum ferric silicate sulfate, 2-3 parts of CITREM, 4-6 parts of alkali lignin and 8-10 parts of antimicrobial powder. With addition of glass flake, tea dust and calcium hexaboride, chemical corrosion resistance and ageing resistance of ceramic tiles can be enhanced. In addition, with addition of konjaku flour, soya lecithin, poly-aluminum ferric silicate sulfate and the like, adhesive stress among mineral particles can be raised, and ageing cracking of ceramic tiles can be prevented effectively. The prepared ceramic bowl has excellent heat resistance, corrosion resistance and ageing resistance, is not easy to crack or break and has long service life.
Ageing cracking resistant ceramic bowl and preparation method thereof
SHU XIAOSHAN (author) / ZHANG JIANWU (author) / GONG PING (author) / TANG XINGYOU (author)
2015-09-30
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Wear-resistant ceramic bowl and preparation method thereof
European Patent Office | 2015
|Medicinal mineral ceramic bowl and preparation method thereof
European Patent Office | 2015
|High-strength ceramic bowl and preparation method thereof
European Patent Office | 2015
|