The invention discloses a quartz anti-cracking refractory material, which is composed of the following raw materials by weight part: 3-6 of terpene resin, 0.2-0.3 of Sp-80, 10-14 of clay, 13-20 of chromium oxide, 50-70 of fused quartz, 10-13 of zirconium silicate, 2-3 of asphalt, 0.1-0.16 of polyvinyl alcohol, 0.4-1 of lanolin, 10-16 of flax fiber, 2-3 of glacial acetic acid, 26-30 of tetraethyl orthosilicate, 80-102 of 6-10% ammonia water, 100-110 of 3-5% hydrogen peroxide, and 0.4-1 of potassium dihydrogen phosphate. The tetraethyl orthosilicate involved in the invention is hydrolyzed into silanol sol under the condition of adding the catalyst glacial acetic acid, the silanol sol is mixed with a fiber activation solution, and by evaporation of the solvent, a heterocomplex containing carbon and silicon can be obtained, and finally high temperature carbonization is carried out, and the carbon source is provided by the fiber activation solution, thus obtaining a carbon silicon composite additive. The carbon silicon composite additive has the advantages of stable chemical properties, high heat conductivity coefficient, small thermal expansion coefficient, thermal shock resistance, light weight, and high strength.
The invention discloses a quartz anti-cracking refractory material, which is composed of the following raw materials by weight part: 3-6 of terpene resin, 0.2-0.3 of Sp-80, 10-14 of clay, 13-20 of chromium oxide, 50-70 of fused quartz, 10-13 of zirconium silicate, 2-3 of asphalt, 0.1-0.16 of polyvinyl alcohol, 0.4-1 of lanolin, 10-16 of flax fiber, 2-3 of glacial acetic acid, 26-30 of tetraethyl orthosilicate, 80-102 of 6-10% ammonia water, 100-110 of 3-5% hydrogen peroxide, and 0.4-1 of potassium dihydrogen phosphate. The tetraethyl orthosilicate involved in the invention is hydrolyzed into silanol sol under the condition of adding the catalyst glacial acetic acid, the silanol sol is mixed with a fiber activation solution, and by evaporation of the solvent, a heterocomplex containing carbon and silicon can be obtained, and finally high temperature carbonization is carried out, and the carbon source is provided by the fiber activation solution, thus obtaining a carbon silicon composite additive. The carbon silicon composite additive has the advantages of stable chemical properties, high heat conductivity coefficient, small thermal expansion coefficient, thermal shock resistance, light weight, and high strength.
European Patent Office | 2021
|High-temperature-resistant anti-cracking artificial quartz plate and preparation method thereof
European Patent Office | 2020
|Anti-oxidation refractory material and preparation method thereof
European Patent Office | 2015
|