Antibacterial durable aerated brick and preparation method thereof
The invention discloses an antibacterial durable aerated brick and a preparation method thereof. The antibacterial durable aerated brick is prepared from, by weight, 30-40 parts of yellow phosphorus slags, 25-30 parts of iron ore tailings, 10-15 parts of titanium white gypsum, 8-10 parts of cement, 15-20 parts of treasure sand, 30-35 parts of quartz sand, 5-8 parts ofzeolite powder, 3-5 parts of Chinese medicine residues, 2-3 parts of tea seed shells, 1-3 parts of Arabic gum, 0.5-0.8 part of waste engine oil, 0.3-0.5 part of stearin, 0.5-1 part of zinc stearate, 0.5-1 part of calcium stearate, 1-3 parts of polyethylene glycol, 1-2 parts of propylene glycol amine, 2-3 parts of sodium molybdate, 1-3 parts of calcium sulfate and 1-2 parts of carboxymethyl chitosan. According to the antibacterial durable aerated brick and the preparation method thereof, the aerated brick has a good antibacterial effect through good cooperation of different components, the durability, strength and dry shrinkage resistance are improved, good sound insulation and heat preservation effects are achieved, and the antibacterial durable aerated brick is superior to existing products in the current market.
Antibacterial durable aerated brick and preparation method thereof
The invention discloses an antibacterial durable aerated brick and a preparation method thereof. The antibacterial durable aerated brick is prepared from, by weight, 30-40 parts of yellow phosphorus slags, 25-30 parts of iron ore tailings, 10-15 parts of titanium white gypsum, 8-10 parts of cement, 15-20 parts of treasure sand, 30-35 parts of quartz sand, 5-8 parts ofzeolite powder, 3-5 parts of Chinese medicine residues, 2-3 parts of tea seed shells, 1-3 parts of Arabic gum, 0.5-0.8 part of waste engine oil, 0.3-0.5 part of stearin, 0.5-1 part of zinc stearate, 0.5-1 part of calcium stearate, 1-3 parts of polyethylene glycol, 1-2 parts of propylene glycol amine, 2-3 parts of sodium molybdate, 1-3 parts of calcium sulfate and 1-2 parts of carboxymethyl chitosan. According to the antibacterial durable aerated brick and the preparation method thereof, the aerated brick has a good antibacterial effect through good cooperation of different components, the durability, strength and dry shrinkage resistance are improved, good sound insulation and heat preservation effects are achieved, and the antibacterial durable aerated brick is superior to existing products in the current market.
Antibacterial durable aerated brick and preparation method thereof
SHEN SHENGXIANG (author) / LI FENGBI (author)
2016-01-06
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Mineral powder aerated brick and preparation method thereof
European Patent Office | 2021
|