Slow-release plastic expanding agent for cement-based binding material and preparation method of slow-release plastic expanding agent
The invention provides a slow-release plastic expanding agent for a cement-based binding material and a preparation method of the slow-release plastic expanding agent and particularly relates to a plastic expanding agent capable of continuously generating certain expansion to compensate for early shrinkage of the cement-based binding material before the stage that a cement-based binding material mixture loses plasticity. The slow-release plastic expanding agent for the cement-based binding material is prepared from, by weight, 30-50 parts of aliphatic azo compounds, 20-40 parts of N-nitro compounds, 5-20 parts of foaming promoter and 5-15 parts of foam stabilizer. When the slow-release plastic expanding agent, polycarboxylate water reducing agent, a naphthalene water reducing agent and an aliphatic water reducing agent are compounded for use, the viscosity of the cement-based binding material mixture is slightly increased, the workability of the mixture is improved, micro-expansion is generated, and early shrinkage of the cement-based binding material mixture can be offset to a certain degree.
Slow-release plastic expanding agent for cement-based binding material and preparation method of slow-release plastic expanding agent
The invention provides a slow-release plastic expanding agent for a cement-based binding material and a preparation method of the slow-release plastic expanding agent and particularly relates to a plastic expanding agent capable of continuously generating certain expansion to compensate for early shrinkage of the cement-based binding material before the stage that a cement-based binding material mixture loses plasticity. The slow-release plastic expanding agent for the cement-based binding material is prepared from, by weight, 30-50 parts of aliphatic azo compounds, 20-40 parts of N-nitro compounds, 5-20 parts of foaming promoter and 5-15 parts of foam stabilizer. When the slow-release plastic expanding agent, polycarboxylate water reducing agent, a naphthalene water reducing agent and an aliphatic water reducing agent are compounded for use, the viscosity of the cement-based binding material mixture is slightly increased, the workability of the mixture is improved, micro-expansion is generated, and early shrinkage of the cement-based binding material mixture can be offset to a certain degree.
Slow-release plastic expanding agent for cement-based binding material and preparation method of slow-release plastic expanding agent
KE KAI (author) / JIANG BO (author) / HE XINGYANG (author) / SU YING (author) / CHANG YING (author) / SUN YIHENG (author) / DAI FEI (author)
2016-01-27
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2023
|Preparation method of slow-release water reducing agent for cement
European Patent Office | 2020
|European Patent Office | 2024
|Cement base material expanding agent and preparation method thereof
European Patent Office | 2015
|European Patent Office | 2015
|