Cement kiln tertiary air duct prefabricated member
The invention relates to the field of refractory materials, in particular to a cement kiln tertiary air duct prefabricated member. The cement kiln tertiary air duct prefabricated member is prepared from, by weight, 20-50 parts of white corundum, 18-30 parts of mullite M, 15-40 parts of electric smelting magnesium aluminate spinel, 10-30 parts of electric smelting hercynite, 3-5 parts of zirconium carbonate, 3-5 parts of silicon carbide, 2-3 parts of silica powder, 2-8 parts of alumina micro powder, 0.1-1 part of sodium tripolyphosphate and 5-10 parts of an additional binding agent. The electric smelting magnesium aluminate spinel comprises 15-25 parts of 5-8 mm electric smelting magnesium aluminate spinel granules, 5-20 parts of 3-5 mm electric smelting magnesium aluminate spinel granules, 5-15 parts of 1-3 mm electric smelting magnesium aluminate spinel granules and 5-15 parts of 0-1 mm electric smelting magnesium aluminate spinel granules. The electric smelting hercynite comprises 10-20 parts of 5-8 mm electric smelting hercynite granules, 5-15 parts of 3-5 mm electric smelting hercynite granules, 5-10 parts of 1-3 mm electric smelting hercynite granules and 5-10 parts of 0-1 mm electric smelting hercynite granules. A preparation method of the prefabricated member comprises the steps of preparing a stirring material A, preparing a mixture B, preparing a sample tertiary air duct prefabricated member, preparing a first tertiary air duct prefabricated member, preparing a second tertiary air duct prefabricated member and preparing a final tertiary air duct prefabricated member. The cement kiln tertiary air duct prefabricated member is high in castable wear-resisting property, good in high temperature resistance and high in thermal shock resistance.
Cement kiln tertiary air duct prefabricated member
The invention relates to the field of refractory materials, in particular to a cement kiln tertiary air duct prefabricated member. The cement kiln tertiary air duct prefabricated member is prepared from, by weight, 20-50 parts of white corundum, 18-30 parts of mullite M, 15-40 parts of electric smelting magnesium aluminate spinel, 10-30 parts of electric smelting hercynite, 3-5 parts of zirconium carbonate, 3-5 parts of silicon carbide, 2-3 parts of silica powder, 2-8 parts of alumina micro powder, 0.1-1 part of sodium tripolyphosphate and 5-10 parts of an additional binding agent. The electric smelting magnesium aluminate spinel comprises 15-25 parts of 5-8 mm electric smelting magnesium aluminate spinel granules, 5-20 parts of 3-5 mm electric smelting magnesium aluminate spinel granules, 5-15 parts of 1-3 mm electric smelting magnesium aluminate spinel granules and 5-15 parts of 0-1 mm electric smelting magnesium aluminate spinel granules. The electric smelting hercynite comprises 10-20 parts of 5-8 mm electric smelting hercynite granules, 5-15 parts of 3-5 mm electric smelting hercynite granules, 5-10 parts of 1-3 mm electric smelting hercynite granules and 5-10 parts of 0-1 mm electric smelting hercynite granules. A preparation method of the prefabricated member comprises the steps of preparing a stirring material A, preparing a mixture B, preparing a sample tertiary air duct prefabricated member, preparing a first tertiary air duct prefabricated member, preparing a second tertiary air duct prefabricated member and preparing a final tertiary air duct prefabricated member. The cement kiln tertiary air duct prefabricated member is high in castable wear-resisting property, good in high temperature resistance and high in thermal shock resistance.
Cement kiln tertiary air duct prefabricated member
WANG QIANG (author) / XU GAO (author) / SHAN GUOQIANG (author)
2016-01-27
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Tertiary air duct curve prefabricated component for cement kiln
European Patent Office | 2015
|Preparation method of tertiary air duct curve prefabricated component used for cement kiln
European Patent Office | 2015
|High-performance alkali-resistant bricks for cement rotary kiln tertiary air duct
European Patent Office | 2015
|