Preparation method for architectural decoration flambe art ceramic tile
The invention discloses a preparation method for an architectural decoration flambe art ceramic tile. Ground coat is prepared from, by weight, 14%-19% of potassium feldspar+albite, 10%-15% of porcelain sand, 5%-10% of kaolin, 5%-12% of zinc oxide, 5%-10% of calcined talc, 15%-20% of barium carbonate, 3%-8% of dolomite, 11%-16% of calcium carbonate, 3%-10% of calcium phosphate and 2%-7% of aluminum oxide. Cover glaze is prepared from, by weight, 16%-23% of feldspar+albite, 5%-10% of porcelain sand, 5%-10% of kaolin, 17%-23% of zinc oxide, 5%-10% of calcined talc, 10%-16% of zirconium silicate, 14%-18% of titanium oxide, 5%-10% of glass dust and 1%-2% of colorant. The architectural decoration flambe art ceramic tile is formed through the steps of burdening, pulping, powder making, press forming, drying, ground coat sprinkling, cover glaze sprinkling, firing, fine trimming packaging and the like. The apparent size of snowflake-shaped crystal patterns ranges from 3 mm to 6 mm, and the maximum apparent size of cotton-shaped crystal patterns can reach about 20 mm. Low-temperature rapid sintering of flambe art ceramic is achieved, firing cost is reduced, and energy saving, consumption reduction and emission reduction are achieved.
Preparation method for architectural decoration flambe art ceramic tile
The invention discloses a preparation method for an architectural decoration flambe art ceramic tile. Ground coat is prepared from, by weight, 14%-19% of potassium feldspar+albite, 10%-15% of porcelain sand, 5%-10% of kaolin, 5%-12% of zinc oxide, 5%-10% of calcined talc, 15%-20% of barium carbonate, 3%-8% of dolomite, 11%-16% of calcium carbonate, 3%-10% of calcium phosphate and 2%-7% of aluminum oxide. Cover glaze is prepared from, by weight, 16%-23% of feldspar+albite, 5%-10% of porcelain sand, 5%-10% of kaolin, 17%-23% of zinc oxide, 5%-10% of calcined talc, 10%-16% of zirconium silicate, 14%-18% of titanium oxide, 5%-10% of glass dust and 1%-2% of colorant. The architectural decoration flambe art ceramic tile is formed through the steps of burdening, pulping, powder making, press forming, drying, ground coat sprinkling, cover glaze sprinkling, firing, fine trimming packaging and the like. The apparent size of snowflake-shaped crystal patterns ranges from 3 mm to 6 mm, and the maximum apparent size of cotton-shaped crystal patterns can reach about 20 mm. Low-temperature rapid sintering of flambe art ceramic is achieved, firing cost is reduced, and energy saving, consumption reduction and emission reduction are achieved.
Preparation method for architectural decoration flambe art ceramic tile
LIAO YONGKANG (author)
2016-02-10
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Ceramic tile cement smearing device for architectural decoration
European Patent Office | 2020
|Preparation method of novel flambe rainforest blue glaze ceramic container
European Patent Office | 2020
|Ceramic tile with mirror relief decoration effect and preparation method of ceramic tile
European Patent Office | 2022
|Tendances - L'environnement certifié. L'acier flambe.
Online Contents | 2004