The invention discloses ceramic overglazed pearly luster embossment color decal paper and a manufacturing method thereof. The ceramic overglazed pearly luster embossment color decal paper is made of raw materials including, by mass part, 10 to 20 parts of feldspar powder, 20 to 25 parts of low-temperature lead-free frit, 50 to 80 parts of pearl powder, 2 to 8 parts of aluminum oxide, 20 to 30 parts of overglazed transparent white colour modulation slurry, 3 to 8 parts of zirconium silicate, 40 to 75 parts of ethyl alcohol, 55 to 85 parts of ink, 40 to 60 parts of water, 10 to 12 parts of ammonium fluozirconate, 2 to 5 parts of sodium hexametaphosphate, 15 to 20 parts of zinc silicofluoride, 5 to 10 parts of ammonium borofluoride, 1 to 5 parts of silver nitrate, 5 to 10 parts of lanthanum nitrate, 24 to 43 parts of auxiliary materials, 27 to 51 parts of oxidation compositions and 0.8 to 1.4 parts of an additive. The ceramic overglazed pearly luster embossment color decal paper has the beneficial effects that the yield of decoration of the paper on a ceramic product can be achieved, no defects exist, more attractiveness is achieved, the hand feeling is more rich, and the lead and cadmium dissolving-out amount can meet the national standards of the Europe and America.
本发明公开了一种陶瓷釉上珠光浮雕彩花纸及其制作方法,该陶瓷釉上珠光浮雕彩花纸由以下质量份数的原料制成:长石粉10‑20份、低温无铅熔块20‑25份、珠光粉50‑80份、氧化铝2‑8份、釉上透明调色白20‑30份、硅酸锆3‑8份、乙醇40‑75份、油墨55‑85份,水40‑60份、六氟合锆酸铵10‑12份,六偏磷酸钠2‑5份,六氟硅酸锌15‑20份,氟硼酸铵5‑10份,硝酸银1‑5份,硝酸镧5‑10份、辅料24‑43份、氧化组合物27‑51份和添加剂0.8‑1.4份。有益效果:实现了其装饰在陶瓷产品上的成品率高,无暇庇,更美观,手感更丰富;并且铅镉溶出量可达到欧美等国家标准。
The invention discloses ceramic overglazed pearly luster embossment color decal paper and a manufacturing method thereof. The ceramic overglazed pearly luster embossment color decal paper is made of raw materials including, by mass part, 10 to 20 parts of feldspar powder, 20 to 25 parts of low-temperature lead-free frit, 50 to 80 parts of pearl powder, 2 to 8 parts of aluminum oxide, 20 to 30 parts of overglazed transparent white colour modulation slurry, 3 to 8 parts of zirconium silicate, 40 to 75 parts of ethyl alcohol, 55 to 85 parts of ink, 40 to 60 parts of water, 10 to 12 parts of ammonium fluozirconate, 2 to 5 parts of sodium hexametaphosphate, 15 to 20 parts of zinc silicofluoride, 5 to 10 parts of ammonium borofluoride, 1 to 5 parts of silver nitrate, 5 to 10 parts of lanthanum nitrate, 24 to 43 parts of auxiliary materials, 27 to 51 parts of oxidation compositions and 0.8 to 1.4 parts of an additive. The ceramic overglazed pearly luster embossment color decal paper has the beneficial effects that the yield of decoration of the paper on a ceramic product can be achieved, no defects exist, more attractiveness is achieved, the hand feeling is more rich, and the lead and cadmium dissolving-out amount can meet the national standards of the Europe and America.
本发明公开了一种陶瓷釉上珠光浮雕彩花纸及其制作方法,该陶瓷釉上珠光浮雕彩花纸由以下质量份数的原料制成:长石粉10‑20份、低温无铅熔块20‑25份、珠光粉50‑80份、氧化铝2‑8份、釉上透明调色白20‑30份、硅酸锆3‑8份、乙醇40‑75份、油墨55‑85份,水40‑60份、六氟合锆酸铵10‑12份,六偏磷酸钠2‑5份,六氟硅酸锌15‑20份,氟硼酸铵5‑10份,硝酸银1‑5份,硝酸镧5‑10份、辅料24‑43份、氧化组合物27‑51份和添加剂0.8‑1.4份。有益效果:实现了其装饰在陶瓷产品上的成品率高,无暇庇,更美观,手感更丰富;并且铅镉溶出量可达到欧美等国家标准。
Ceramic overglazed pearly luster embossment color decal paper and manufacturing method thereof
一种陶瓷釉上珠光浮雕彩花纸及其制作方法
SU XIBAN (author)
2020-04-28
Patent
Electronic Resource
Chinese
Ceramic tile with embossment effect and preparation method thereof
European Patent Office | 2022
|MANUFACTURING METHOD OF OVERGLAZED PORCELAIN WITH PATTERNS USING LASER
European Patent Office | 2016
|