Water-based epoxy anti-static floor bottom and middle coating and construction process thereof
The invention relates to a water-based epoxy anti-static floor bottom and middle coating and a construction process thereof. The water-based epoxy anti-static floor bottom and middle coating is composed of a component A and a component B. The component A is composed of the following components in percentage by mass: 20-30% of a II-generation water-based epoxy resin curing agent; 40-59 percent of water; and 0.1-1% of a dispersant. The component B is composed of bisphenol A epoxy resin and an active diluent, and is characterized by further comprising composite conductive resin, the composite conductive resin is compounded with conductive graphite powder or metal powder, and the total volume ratio of the composite resin to the component A to the component B is 1:10-1:5. During construction, when grinding particles are used, a spraying process is adopted, the composite resin is ground and sprayed with liquid in a one-way mode, and when the light-cured resin is used, the light-cured resin is sprayed firstly, and then the component A and the component B are sprayed after semi-curing. The coating and the process can ensure that the wire is uniform and the anti-static effect is stable.
一种水性环氧防静电地坪底、中涂涂料及其施工工艺,一种水性环氧防静电地坪底、中涂涂料,由甲乙两组分组成,甲组分由以下质量百分比组分组成:II代水性环氧树脂固化剂20~30%;水40~59%;分散剂0.1~1%;乙组分由双酚A型环氧树脂和活性稀释剂组成,其特征在于,还包括复合导电树脂,复合导电树脂复合导电石墨粉或金属粉,复合树脂与甲乙组份总体积比例为1:10‑1:5。施工上,当使用的是粉磨颗粒时采用喷涂工艺,将复合树脂粉磨与液体一通喷涂,当使用光固化树脂时,先喷涂光固化树脂,半固化后在喷涂甲乙组份。该涂料和工艺能够确保导线均匀,防静电效果稳定。
Water-based epoxy anti-static floor bottom and middle coating and construction process thereof
The invention relates to a water-based epoxy anti-static floor bottom and middle coating and a construction process thereof. The water-based epoxy anti-static floor bottom and middle coating is composed of a component A and a component B. The component A is composed of the following components in percentage by mass: 20-30% of a II-generation water-based epoxy resin curing agent; 40-59 percent of water; and 0.1-1% of a dispersant. The component B is composed of bisphenol A epoxy resin and an active diluent, and is characterized by further comprising composite conductive resin, the composite conductive resin is compounded with conductive graphite powder or metal powder, and the total volume ratio of the composite resin to the component A to the component B is 1:10-1:5. During construction, when grinding particles are used, a spraying process is adopted, the composite resin is ground and sprayed with liquid in a one-way mode, and when the light-cured resin is used, the light-cured resin is sprayed firstly, and then the component A and the component B are sprayed after semi-curing. The coating and the process can ensure that the wire is uniform and the anti-static effect is stable.
一种水性环氧防静电地坪底、中涂涂料及其施工工艺,一种水性环氧防静电地坪底、中涂涂料,由甲乙两组分组成,甲组分由以下质量百分比组分组成:II代水性环氧树脂固化剂20~30%;水40~59%;分散剂0.1~1%;乙组分由双酚A型环氧树脂和活性稀释剂组成,其特征在于,还包括复合导电树脂,复合导电树脂复合导电石墨粉或金属粉,复合树脂与甲乙组份总体积比例为1:10‑1:5。施工上,当使用的是粉磨颗粒时采用喷涂工艺,将复合树脂粉磨与液体一通喷涂,当使用光固化树脂时,先喷涂光固化树脂,半固化后在喷涂甲乙组份。该涂料和工艺能够确保导线均匀,防静电效果稳定。
Water-based epoxy anti-static floor bottom and middle coating and construction process thereof
一种水性环氧防静电地坪底、中涂涂料及其施工工艺
HAN BIN (author) / HAN MINGRUI (author)
2020-05-05
Patent
Electronic Resource
Chinese
Waterborne epoxy anti-static floor bottom and middle coating and construction method thereof
European Patent Office | 2020
|Anti-static epoxy floor construction process and coating equipment thereof
European Patent Office | 2023
|Non-ignition anti-static terrazzo floor and construction process thereof
European Patent Office | 2022
|