Method for preparing geopolymer cementing material from regenerated micro-powder
The invention discloses a method for preparing a geopolymer cementing material from regenerated micro-powder. The cementing material is obtained by mixing geopolymer powder and an alkali activator, carrying out stirring for a period of time, molding obtained slurry, and carrying out standard maintenance, wherein the geopolymer powder comprises 30-70 wt% of slag powder and 30-70 wt% of regeneratedmicro-powder. The geopolymer cementing material prepared by the invention has high strength and good contractibility and can solve the problem of contraction cracking of common concrete materials; meanwhile, the regenerated micro-powder is used as a raw material, so construction waste is effectively utilized; and the method is a green and environment-friendly method.
本发明公开了一种采用再生微粉制备地聚合物胶凝材料的方法,所述胶凝材料通过将地聚合物粉体和碱激发剂混合后搅拌一段时间,所得浆体成型、标准养护后得到,其中,地聚合物粉体由30~70wt%矿渣粉、30~70wt%再生微粉组成。本发明制备的地聚合物胶凝材料,具有较高的强度,且收缩性良好,可以解决常见混凝土材料收缩开裂的问题,同时,本发明以再生微粉为原料,有效利用了建筑垃圾,是一种绿色环保的方法。
Method for preparing geopolymer cementing material from regenerated micro-powder
The invention discloses a method for preparing a geopolymer cementing material from regenerated micro-powder. The cementing material is obtained by mixing geopolymer powder and an alkali activator, carrying out stirring for a period of time, molding obtained slurry, and carrying out standard maintenance, wherein the geopolymer powder comprises 30-70 wt% of slag powder and 30-70 wt% of regeneratedmicro-powder. The geopolymer cementing material prepared by the invention has high strength and good contractibility and can solve the problem of contraction cracking of common concrete materials; meanwhile, the regenerated micro-powder is used as a raw material, so construction waste is effectively utilized; and the method is a green and environment-friendly method.
本发明公开了一种采用再生微粉制备地聚合物胶凝材料的方法,所述胶凝材料通过将地聚合物粉体和碱激发剂混合后搅拌一段时间,所得浆体成型、标准养护后得到,其中,地聚合物粉体由30~70wt%矿渣粉、30~70wt%再生微粉组成。本发明制备的地聚合物胶凝材料,具有较高的强度,且收缩性良好,可以解决常见混凝土材料收缩开裂的问题,同时,本发明以再生微粉为原料,有效利用了建筑垃圾,是一种绿色环保的方法。
Method for preparing geopolymer cementing material from regenerated micro-powder
一种采用再生微粉制备地聚合物胶凝材料的方法
WU ZHENGGUANG (author) / LIU CONG (author) / XIAO PENG (author) / KANG AIHONG (author) / LIU AN'AN (author) / SUN HAIFENG (author)
2020-05-12
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2024
|European Patent Office | 2021
|Method for preparing regenerated cementing material by using waste concrete
European Patent Office | 2022
|Pickling purification equipment for preparing regenerated cementing material from waste concrete
European Patent Office | 2023
|European Patent Office | 2021
|