The invention discloses a durable environment-friendly building block brick and a preparation method thereof. The durable environment-friendly building block brick is prepared from the following raw materials in parts by weight: 3.5-5.5 parts of cement, 5.5-8.5 parts of modified montmorillonite, 8.0-12.0 parts of ceramsite, 6.0-9.0 parts of waste rock slag, 6.0-8.0 parts of kaolin, 3.0-4.0 parts of mica, 1.0-3.0 parts of glass fibers, 0.8-1.8 parts of polyurethane fibers, 4.5-8.5 parts of nano silicon dioxide, 2.2-4.2 parts of polyacrylamide and 1.2-1.8 parts of ethylene glycol. According to the durable environment-friendly building block brick, a traditional formula is improved, the modified montmorillonite, the glass fibers, the polyester fibers and the like are added, and all the components act together and supplement one another, so that the abrasion resistance and the compression resistance degree of the building block brick can be obviously improved, the use safety and the economic value of the building block brick are improved, and the service life of the building block brick is prolonged.
本发明公开了一种耐用环保积木砖及其制备方法,所述耐用环保积木砖由以下重量份的原料组成:水泥3.5份~5.5份、改性蒙脱土5.5份~8.5份、陶粒8.0份~12.0份、废石渣6.0份~9.0份、高岭土6.0份~8.0份、云母3.0份~4.0份、玻璃纤维1.0份~3.0份、聚氨酯纤维0.8份~1.8份、纳米二氧化硅4.5份~8.5份、聚丙烯酰胺2.2份~4.2份、乙二醇1.2份~1.8份。本发明耐用环保积木砖,对传统配方进行改进,添加改性蒙脱土、玻璃纤维和聚酯纤维等,各组分共同作用,相辅相成,可以明显改善积木砖的耐磨性和抗压程度,提高积木砖的使用安全性和经济价值,延长使用寿命。
The invention discloses a durable environment-friendly building block brick and a preparation method thereof. The durable environment-friendly building block brick is prepared from the following raw materials in parts by weight: 3.5-5.5 parts of cement, 5.5-8.5 parts of modified montmorillonite, 8.0-12.0 parts of ceramsite, 6.0-9.0 parts of waste rock slag, 6.0-8.0 parts of kaolin, 3.0-4.0 parts of mica, 1.0-3.0 parts of glass fibers, 0.8-1.8 parts of polyurethane fibers, 4.5-8.5 parts of nano silicon dioxide, 2.2-4.2 parts of polyacrylamide and 1.2-1.8 parts of ethylene glycol. According to the durable environment-friendly building block brick, a traditional formula is improved, the modified montmorillonite, the glass fibers, the polyester fibers and the like are added, and all the components act together and supplement one another, so that the abrasion resistance and the compression resistance degree of the building block brick can be obviously improved, the use safety and the economic value of the building block brick are improved, and the service life of the building block brick is prolonged.
本发明公开了一种耐用环保积木砖及其制备方法,所述耐用环保积木砖由以下重量份的原料组成:水泥3.5份~5.5份、改性蒙脱土5.5份~8.5份、陶粒8.0份~12.0份、废石渣6.0份~9.0份、高岭土6.0份~8.0份、云母3.0份~4.0份、玻璃纤维1.0份~3.0份、聚氨酯纤维0.8份~1.8份、纳米二氧化硅4.5份~8.5份、聚丙烯酰胺2.2份~4.2份、乙二醇1.2份~1.8份。本发明耐用环保积木砖,对传统配方进行改进,添加改性蒙脱土、玻璃纤维和聚酯纤维等,各组分共同作用,相辅相成,可以明显改善积木砖的耐磨性和抗压程度,提高积木砖的使用安全性和经济价值,延长使用寿命。
Durable environment-friendly building block brick and preparation method thereof
一种耐用环保积木砖及其制备方法
2020-06-19
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly durable mixed type sintered hollow brick and preparation method thereof
European Patent Office | 2015
|Mixed type environment-friendly durable non-burnt hollow brick and preparation method thereof
European Patent Office | 2015
|Building waste environment-friendly recycled brick and preparation method thereof
European Patent Office | 2021
|Novel environment-friendly building material brick and preparation method thereof
European Patent Office | 2021
|Environment-friendly brick and preparation method thereof
European Patent Office | 2021
|