Mixed type environment-friendly durable non-burnt hollow brick and preparation method thereof
The invention discloses a mixed type environment-friendly durable non-burnt hollow brick, which is characterized by being prepared from the following raw materials by weight part: 11-13 of ordinary cement, 0.9-1.2 of sodium lignin sulfonate, 15-18 of quicklime, 1-2 of rosin soap, 0.4-0.7 of tea saponin, 0.4-0.6 of 107 glue, 30-34 of shale, 28-31 of yellow phosphorus slag, 11-14 of honeycomb cinder, 3-4.5 of waterborne polyurethane, 15-18 of a synergist, and a proper amount of water. The non-burnt hollow brick provided by the invention is added with yellow phosphorus slag, honeycomb cinder and the like, utilizes waste materials, and is energy saving and environment-friendly. The synergist made by special technique has the characteristics of light weight, high strength, water resistance, thermal insulation, bacteria resistance, and mildew prevention. The 107 glue and waterborne polyurethane are added for cooperation, thus enhancing the strength, toughness, durability and ageing resistance of the product. According to the invention, the process is simple, and convenient to operate, and the non-burnt hollow brick has the advantages of low investment cost, small heat transfer coefficient, high strength, corrosion resistance, and is worthy of large area promotion and application.
Mixed type environment-friendly durable non-burnt hollow brick and preparation method thereof
The invention discloses a mixed type environment-friendly durable non-burnt hollow brick, which is characterized by being prepared from the following raw materials by weight part: 11-13 of ordinary cement, 0.9-1.2 of sodium lignin sulfonate, 15-18 of quicklime, 1-2 of rosin soap, 0.4-0.7 of tea saponin, 0.4-0.6 of 107 glue, 30-34 of shale, 28-31 of yellow phosphorus slag, 11-14 of honeycomb cinder, 3-4.5 of waterborne polyurethane, 15-18 of a synergist, and a proper amount of water. The non-burnt hollow brick provided by the invention is added with yellow phosphorus slag, honeycomb cinder and the like, utilizes waste materials, and is energy saving and environment-friendly. The synergist made by special technique has the characteristics of light weight, high strength, water resistance, thermal insulation, bacteria resistance, and mildew prevention. The 107 glue and waterborne polyurethane are added for cooperation, thus enhancing the strength, toughness, durability and ageing resistance of the product. According to the invention, the process is simple, and convenient to operate, and the non-burnt hollow brick has the advantages of low investment cost, small heat transfer coefficient, high strength, corrosion resistance, and is worthy of large area promotion and application.
Mixed type environment-friendly durable non-burnt hollow brick and preparation method thereof
ZHU CHUN (author) / ZHU SHIJUN (author)
2015-09-09
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Environment-friendly durable mixed type sintered hollow brick and preparation method thereof
European Patent Office | 2015
|Durable environment-friendly building block brick and preparation method thereof
European Patent Office | 2020
|Synergist added non-burnt hollow brick and preparation method thereof
European Patent Office | 2015
|Environment-friendly high-toughness hollow brick and preparation method thereof
European Patent Office | 2023
|