Anti-crack concrete and preparation method thereof as well as anti-crack assembly type prefabricated component composite floor slab and preparation method thereof
The invention relates to the technical field of composite floor slabs, in particular to anti-crack concrete, a preparation method thereof, an anti-crack assembly type prefabricated component compositefloor slab and a preparation method thereof. The anti-crack concrete provided by the invention is prepared from the following preparation raw materials in parts by weight: 270 to 300 parts of cement,70 to 100 parts of fly ash, 850 to 900 parts of sand, 1000 to 1150 parts of stone, 5.5 to 6.2 parts of a water reducing agent, 0.8 to 1.0 part of a waterproof agent and 160 to 170 parts of water. Theanti-crack effect of the concrete can be improved through the matching effect of all the components and the dosage.
本发明涉及叠合楼板技术领域,具体涉及一种抗裂混凝土及其制备方法和一种抗裂型装配式预制构件叠合楼板及其制备方法。本发明提供的抗裂混凝土,按重量份数计,包括以下组分的制备原料:水泥270~300份,粉煤灰70~100份,砂子850~900份,石子1000~1150份,减水剂5.5~6.2份,防水剂0.8~1.0份,水160~170份。本发明通过各组分以及用量的配合作用,能够提高混凝土的抗裂效果。
Anti-crack concrete and preparation method thereof as well as anti-crack assembly type prefabricated component composite floor slab and preparation method thereof
The invention relates to the technical field of composite floor slabs, in particular to anti-crack concrete, a preparation method thereof, an anti-crack assembly type prefabricated component compositefloor slab and a preparation method thereof. The anti-crack concrete provided by the invention is prepared from the following preparation raw materials in parts by weight: 270 to 300 parts of cement,70 to 100 parts of fly ash, 850 to 900 parts of sand, 1000 to 1150 parts of stone, 5.5 to 6.2 parts of a water reducing agent, 0.8 to 1.0 part of a waterproof agent and 160 to 170 parts of water. Theanti-crack effect of the concrete can be improved through the matching effect of all the components and the dosage.
本发明涉及叠合楼板技术领域,具体涉及一种抗裂混凝土及其制备方法和一种抗裂型装配式预制构件叠合楼板及其制备方法。本发明提供的抗裂混凝土,按重量份数计,包括以下组分的制备原料:水泥270~300份,粉煤灰70~100份,砂子850~900份,石子1000~1150份,减水剂5.5~6.2份,防水剂0.8~1.0份,水160~170份。本发明通过各组分以及用量的配合作用,能够提高混凝土的抗裂效果。
Anti-crack concrete and preparation method thereof as well as anti-crack assembly type prefabricated component composite floor slab and preparation method thereof
一种抗裂混凝土及其制备方法和一种抗裂型装配式预制构件叠合楼板及其制备方法
XING LIJUN (author) / LIU XINGHUA (author) / HE CHANGLI (author) / WANG ZHILI (author) / CHANG SHITAO (author) / LU ZAO (author) / LIU YANG (author)
2020-07-07
Patent
Electronic Resource
Chinese
Anti-crack concrete prefabricated part and preparation method thereof
European Patent Office | 2024
|Prefabricated composite floor slab and preparation method thereof
European Patent Office | 2024
|Anti-crack ballastless track roadbed slab concrete and preparation method thereof
European Patent Office | 2023
|High-strength and anti-crack concrete prefabricated part and preparation method thereof
European Patent Office | 2023
|