A platform for research: civil engineering, architecture and urbanism
High-strength heat-preservation autoclaved aerated building block
The invention relates to the technical field of building materials, and relates to a high-strength heat-preservation autoclaved aerated building block which is prepared from the following raw materials in parts by mass: 40-50 parts of water; 20-5 parts of cement; 2-4 parts of a water reducing agent; 0.1-0.3 part of a foaming agent; 50-70 parts of fine aggregate; 3-7 parts of waste fibers; 3-8 parts of waste rubber; and 1-2 parts of 2, 4, 6-trimethylbenzoyl diphenoxyphosphine. The high-strength heat-preservation autoclaved aerated building block has the advantages that the compressive strengthof the high-strength heat-preservation autoclaved aerated building block is improved through the waste, the application range of the high-strength heat-preservation autoclaved aerated building block is wider, and better energy conservation and environmental protection are facilitated and the influence of the waste on the environment is reduced.
本发明涉及建筑材料的技术领域,涉及一种高强保温蒸压加气砌块,其由包含以下质量份数的原料制成:水40‑50份;水泥20‑35份;减水剂2‑4份;发泡剂0.1‑0.3份;细集料50‑70份;废旧纤维3‑7份;废旧橡胶3‑8份;2,4,6‑三甲基苯甲酰二苯氧磷1‑2份。本发明具有利用废弃物提高高强保温蒸压加气砌块的抗压强度,使得高强保温蒸压加气砌块的适用范围更广,同时,有利于更好地节能环保,有利于减少废弃物对环境造成影响的效果。
High-strength heat-preservation autoclaved aerated building block
The invention relates to the technical field of building materials, and relates to a high-strength heat-preservation autoclaved aerated building block which is prepared from the following raw materials in parts by mass: 40-50 parts of water; 20-5 parts of cement; 2-4 parts of a water reducing agent; 0.1-0.3 part of a foaming agent; 50-70 parts of fine aggregate; 3-7 parts of waste fibers; 3-8 parts of waste rubber; and 1-2 parts of 2, 4, 6-trimethylbenzoyl diphenoxyphosphine. The high-strength heat-preservation autoclaved aerated building block has the advantages that the compressive strengthof the high-strength heat-preservation autoclaved aerated building block is improved through the waste, the application range of the high-strength heat-preservation autoclaved aerated building block is wider, and better energy conservation and environmental protection are facilitated and the influence of the waste on the environment is reduced.
本发明涉及建筑材料的技术领域,涉及一种高强保温蒸压加气砌块,其由包含以下质量份数的原料制成:水40‑50份;水泥20‑35份;减水剂2‑4份;发泡剂0.1‑0.3份;细集料50‑70份;废旧纤维3‑7份;废旧橡胶3‑8份;2,4,6‑三甲基苯甲酰二苯氧磷1‑2份。本发明具有利用废弃物提高高强保温蒸压加气砌块的抗压强度,使得高强保温蒸压加气砌块的适用范围更广,同时,有利于更好地节能环保,有利于减少废弃物对环境造成影响的效果。
High-strength heat-preservation autoclaved aerated building block
一种高强保温蒸压加气砌块
HAN XIANGDONG (author) / WU ZHILIN (author) / GONG MINGCHENG (author)
2020-08-14
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Autoclaved aerated concrete block production method and autoclaved aerated concrete block
European Patent Office | 2021
|Pouring forming method for heat preservation type autoclaved aerated concrete block
European Patent Office | 2021
|