High-strength ground repairing mortar
The invention provides a novel high-strength repair mortar. After a formula is optimized, the high-strength repair mortar with high initial setting speed, high initial strength and high self-sealing performance is obtained. The mortar is prepared from, by mass, 300-350 parts of ordinary portland cement, 200-250 parts of sulphoaluminate cement, 50-100 parts of coarse whiting (calcium carbonate), 350 parts of river sand, 1-5 parts of a retarder, 0.5-1 part of fibers, 1-2 parts of hydroxypropyl methyl cellulose, 20-25 parts of rubber powder, 0.5-0.8 part of an organic silicon defoamer, 0.5-0.8 part of an early strength agent, 60-80 parts of gypsum and 220-280 parts of water. The raw materials are weighed, and are stirred for 5 min in a forced physical stirring mode to obtain the slurry-shapedrepairing mortar.
本发明提供了一种新型的高强度修补砂浆,通过优化配方后得出初凝速度快且初始强度高,自密封性强的高强度修补砂浆,本申请砂浆包括了如下质量份的原料,普硅水泥300‑350份,硫铝水泥200‑250份,重钙(碳酸钙)50‑100份,河沙350份,缓凝剂1‑5份,纤维0.5‑1份,羟丙基甲基纤维素1‑2份,胶粉20‑25份,有机硅消泡剂0.5‑0.8份,早强剂0.5‑0.8份,石膏60‑80份,水220‑280份;上述原料在称取完成后,通过强制物理搅拌方式搅拌5min后,得到桨体状的修补砂浆。
High-strength ground repairing mortar
The invention provides a novel high-strength repair mortar. After a formula is optimized, the high-strength repair mortar with high initial setting speed, high initial strength and high self-sealing performance is obtained. The mortar is prepared from, by mass, 300-350 parts of ordinary portland cement, 200-250 parts of sulphoaluminate cement, 50-100 parts of coarse whiting (calcium carbonate), 350 parts of river sand, 1-5 parts of a retarder, 0.5-1 part of fibers, 1-2 parts of hydroxypropyl methyl cellulose, 20-25 parts of rubber powder, 0.5-0.8 part of an organic silicon defoamer, 0.5-0.8 part of an early strength agent, 60-80 parts of gypsum and 220-280 parts of water. The raw materials are weighed, and are stirred for 5 min in a forced physical stirring mode to obtain the slurry-shapedrepairing mortar.
本发明提供了一种新型的高强度修补砂浆,通过优化配方后得出初凝速度快且初始强度高,自密封性强的高强度修补砂浆,本申请砂浆包括了如下质量份的原料,普硅水泥300‑350份,硫铝水泥200‑250份,重钙(碳酸钙)50‑100份,河沙350份,缓凝剂1‑5份,纤维0.5‑1份,羟丙基甲基纤维素1‑2份,胶粉20‑25份,有机硅消泡剂0.5‑0.8份,早强剂0.5‑0.8份,石膏60‑80份,水220‑280份;上述原料在称取完成后,通过强制物理搅拌方式搅拌5min后,得到桨体状的修补砂浆。
High-strength ground repairing mortar
一种高强度地面修补砂浆
GAO ZHENGPING (author) / CUI WENLONG (author) / WANG HENGSUO (author)
2020-08-28
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Repairing method of concrete structure using high-strength polymer mortar and fireproof mortar
European Patent Office | 2016
|Mortar repairing method and mortar repairing and conveying device
European Patent Office | 2024
|WORKING METHOD OF HIGH STRENGTH MORTAR FOR REPAIRING HIGH STRENGTH CONCRETE BUILDING FRAME
European Patent Office | 2017
|European Patent Office | 2015
|