The invention discloses an alkali-free accelerator and a preparation method thereof, and relates to the technical field of accelerator preparation. The concrete admixture is prepared from the following preparation agents: aluminum sulfate, sodium citrate, a polycarboxylate superplasticizer, ammonia water, a thickener and a stabilizer. The preparation agent is prepared from 40%-60% of aluminum sulfate, 5%-10% of sodium citrate, 5%-10% of a polycarboxylate superplasticizer, 5%-10% of ammonia water with the concentration of 15%-25%, 1%-3% of a stabilizer and 1%-2% of a thickener. The ratio of thepreparation agent to the water ranges from 1: 1.1 to 1: 1.3. The accelerator is generated from aluminum sulfate, sodium citrate and ammonia water, does not contain metal ions, and has no corrosivityor pungent smell; by adding the stabilizer, the stability is high, and the adaptability is high; and the manufacturing process is simple, convenient and fast.
本发明公开了一种无碱速凝剂及制备方法,涉及速凝剂制备技术领域。本发明包括如下制备剂:硫酸铝、柠檬酸钠、聚羧酸减水剂、氨水、增稠剂以及稳定剂;制备剂的比例如下:硫酸铝40%‑60%、柠檬酸钠5%‑10%、聚羧酸减水剂5%‑10%、浓度为15%‑25%的氨水5%‑10%、稳定剂1%‑3%以及增稠剂1%‑2%;制备剂与水的比例范围为1:1.1‑1:1.3。本发明通过通过硫酸铝、柠檬酸钠以及氨水生成速凝剂,不含金属离子,无腐蚀性和刺激性气味;通过添加稳定剂,稳定性高、适应性强;且制作程序简单,方便快捷。
The invention discloses an alkali-free accelerator and a preparation method thereof, and relates to the technical field of accelerator preparation. The concrete admixture is prepared from the following preparation agents: aluminum sulfate, sodium citrate, a polycarboxylate superplasticizer, ammonia water, a thickener and a stabilizer. The preparation agent is prepared from 40%-60% of aluminum sulfate, 5%-10% of sodium citrate, 5%-10% of a polycarboxylate superplasticizer, 5%-10% of ammonia water with the concentration of 15%-25%, 1%-3% of a stabilizer and 1%-2% of a thickener. The ratio of thepreparation agent to the water ranges from 1: 1.1 to 1: 1.3. The accelerator is generated from aluminum sulfate, sodium citrate and ammonia water, does not contain metal ions, and has no corrosivityor pungent smell; by adding the stabilizer, the stability is high, and the adaptability is high; and the manufacturing process is simple, convenient and fast.
本发明公开了一种无碱速凝剂及制备方法,涉及速凝剂制备技术领域。本发明包括如下制备剂:硫酸铝、柠檬酸钠、聚羧酸减水剂、氨水、增稠剂以及稳定剂;制备剂的比例如下:硫酸铝40%‑60%、柠檬酸钠5%‑10%、聚羧酸减水剂5%‑10%、浓度为15%‑25%的氨水5%‑10%、稳定剂1%‑3%以及增稠剂1%‑2%;制备剂与水的比例范围为1:1.1‑1:1.3。本发明通过通过硫酸铝、柠檬酸钠以及氨水生成速凝剂,不含金属离子,无腐蚀性和刺激性气味;通过添加稳定剂,稳定性高、适应性强;且制作程序简单,方便快捷。
Fluorine-free alkali-free accelerator and preparation method thereof
European Patent Office | 2022
|Alkali-free liquid accelerator and preparation method thereof
European Patent Office | 2016
|Powdery alkali-free accelerator and preparation method thereof
European Patent Office | 2024
|Liquid alkali-free accelerator and preparation method thereof
European Patent Office | 2020
|Fluoride-free alkali-free accelerator and preparation method thereof
European Patent Office | 2021
|