Pin type porcelain insulator and preparation method thereof
The invention discloses a pin type porcelain insulator and a preparation method thereof and relates to the technical field of insulators; the pin-type porcelain insulator is prepared from the following raw materials in parts by weight: 16-24 parts of mullite12-20 parts of vermiculite, 12-18 parts of clay, 8-16 parts of zeolite powder, 10-18 parts of mica powder, 20-30 parts of allophane, 10-20 parts of medical stone, 2-6 parts of zircon sand, 4-10 parts of diatomite, 1-3 parts of sodium hexametaphosphate, 1-3 parts of nano silicon nitride, 1-5 parts of nano calcium carbonate, 0.8-1.4 parts ofsepiolite fiber, 0.4-1 part of lignin fiber, 1-5 parts of hexamethyldisilazane, 1-5 parts of dimethylformamide and 3-7 parts of vinyltriethoxysilane. The pin type porcelain insulator has the beneficial effects that the raw materials are reasonably matched, and a proper preparation method is adopted, so that the structural strength and breaking strength of the insulator are improved, and the service life of the insulator is prolonged.
本发明公开了一种针式瓷绝缘子及其制备方法,涉及绝缘子技术领域,该针式瓷绝缘子由以下重量份数的原料制成:莫来石16~24份、蛭石12~20份、粘土12~18份、沸石粉8~16份、云母粉10~18份、水铝英石20~30份、麦饭石10~20份、锆英砂2~6份、硅藻土4~10份、六偏磷酸钠1~3份、纳米氮化硅1~3份、纳米碳酸钙1~5份、海泡石纤维0.8~1.4份、木质素纤维0.4~1份、六甲基二硅胺1~5份、二甲基甲酰胺1~5份、乙烯基三乙氧基硅烷3~7份。本发明的有益效果是通过对原料进行合理搭配并采用合适的制备方法,提高了绝缘子的结构强度、抗断裂强度和使用寿命。
Pin type porcelain insulator and preparation method thereof
The invention discloses a pin type porcelain insulator and a preparation method thereof and relates to the technical field of insulators; the pin-type porcelain insulator is prepared from the following raw materials in parts by weight: 16-24 parts of mullite12-20 parts of vermiculite, 12-18 parts of clay, 8-16 parts of zeolite powder, 10-18 parts of mica powder, 20-30 parts of allophane, 10-20 parts of medical stone, 2-6 parts of zircon sand, 4-10 parts of diatomite, 1-3 parts of sodium hexametaphosphate, 1-3 parts of nano silicon nitride, 1-5 parts of nano calcium carbonate, 0.8-1.4 parts ofsepiolite fiber, 0.4-1 part of lignin fiber, 1-5 parts of hexamethyldisilazane, 1-5 parts of dimethylformamide and 3-7 parts of vinyltriethoxysilane. The pin type porcelain insulator has the beneficial effects that the raw materials are reasonably matched, and a proper preparation method is adopted, so that the structural strength and breaking strength of the insulator are improved, and the service life of the insulator is prolonged.
本发明公开了一种针式瓷绝缘子及其制备方法,涉及绝缘子技术领域,该针式瓷绝缘子由以下重量份数的原料制成:莫来石16~24份、蛭石12~20份、粘土12~18份、沸石粉8~16份、云母粉10~18份、水铝英石20~30份、麦饭石10~20份、锆英砂2~6份、硅藻土4~10份、六偏磷酸钠1~3份、纳米氮化硅1~3份、纳米碳酸钙1~5份、海泡石纤维0.8~1.4份、木质素纤维0.4~1份、六甲基二硅胺1~5份、二甲基甲酰胺1~5份、乙烯基三乙氧基硅烷3~7份。本发明的有益效果是通过对原料进行合理搭配并采用合适的制备方法,提高了绝缘子的结构强度、抗断裂强度和使用寿命。
Pin type porcelain insulator and preparation method thereof
一种针式瓷绝缘子及其制备方法
OUYANG QING (author)
2020-09-11
Patent
Electronic Resource
Chinese
High-performance column type porcelain insulator formula and porcelain insulator thereof
European Patent Office | 2023
|Toughening rod type porcelain insulator and preparation method thereof
European Patent Office | 2023
|Toughening column type porcelain insulator and preparation method thereof
European Patent Office | 2021
|Alumina-based porcelain insulator porcelain body and preparation method thereof
European Patent Office | 2024
|Double-disc porcelain insulator and preparation method thereof
European Patent Office | 2021
|