High-pressure grouting ceramic slurry and preparation method thereof
The invention relates to the technical field of ceramics, in particular to high-pressure grouting ceramic slurry and a preparation method thereof. The ceramic slurry comprise a lean raw material groupand a plastic raw material group; wherein the lean raw material group comprises, by weight, 6-13 parts of pyrophyllite, 6-15 parts of Jiangxi chinastone, 3-10 parts of raw ore mica sheets, 2-8 partsof potassium-sodium sand, 2-9 parts of sodium sand and 3-10 parts of waste porcelain; the plastic raw material group comprises 1-8 parts of magnesian mud, 6-15 parts of Fujian kaolin, 4-9 parts of washed mica powder, 2-6 parts of washed black mud, 8-14 parts of Chaozhou washed mud, 3-6 parts of North China Sea white mud and 2-6 parts of raw ore black mud; the ratio of parts by weight of raw materials of the lean raw material group to the plastic raw material group is 0.7-1: 1. The invention further provides the preparation method of the high-pressure grouting ceramic slurry after component optimization, the raw material components are simple, good filterability can be achieved, and the slurry suction speed during high-pressure grouting can be increased.
本发明涉及陶瓷技术领域,尤其涉及一种高压注浆陶瓷浆料及其制备方法。包括脊性原料组和塑性原料组;按照重量份数计算,所述脊性原料组的原料包括:叶腊石6‑13份、江西瓷石6‑15份、原矿云母片3‑10份、钾钠砂2‑8份、钠砂2‑9份和废瓷3‑10份;所述塑性原料组的原料包括:镁质泥1‑8份、福建高岭土6‑15份、水洗云母粉4‑9份、水洗黑泥2‑6份、潮州水洗泥8‑14份、北海白泥3‑6份和原矿黑泥2‑6份;所述脊性原料组与塑性原料组的原料重量份数比为0.7‑1:1。经过成分优化的本发明还提出了所述的高压注浆陶瓷浆料的制备方法,原料成分简单,可以有较好的过滤性,可以提升高压注浆时吸浆速度的速度。
High-pressure grouting ceramic slurry and preparation method thereof
The invention relates to the technical field of ceramics, in particular to high-pressure grouting ceramic slurry and a preparation method thereof. The ceramic slurry comprise a lean raw material groupand a plastic raw material group; wherein the lean raw material group comprises, by weight, 6-13 parts of pyrophyllite, 6-15 parts of Jiangxi chinastone, 3-10 parts of raw ore mica sheets, 2-8 partsof potassium-sodium sand, 2-9 parts of sodium sand and 3-10 parts of waste porcelain; the plastic raw material group comprises 1-8 parts of magnesian mud, 6-15 parts of Fujian kaolin, 4-9 parts of washed mica powder, 2-6 parts of washed black mud, 8-14 parts of Chaozhou washed mud, 3-6 parts of North China Sea white mud and 2-6 parts of raw ore black mud; the ratio of parts by weight of raw materials of the lean raw material group to the plastic raw material group is 0.7-1: 1. The invention further provides the preparation method of the high-pressure grouting ceramic slurry after component optimization, the raw material components are simple, good filterability can be achieved, and the slurry suction speed during high-pressure grouting can be increased.
本发明涉及陶瓷技术领域,尤其涉及一种高压注浆陶瓷浆料及其制备方法。包括脊性原料组和塑性原料组;按照重量份数计算,所述脊性原料组的原料包括:叶腊石6‑13份、江西瓷石6‑15份、原矿云母片3‑10份、钾钠砂2‑8份、钠砂2‑9份和废瓷3‑10份;所述塑性原料组的原料包括:镁质泥1‑8份、福建高岭土6‑15份、水洗云母粉4‑9份、水洗黑泥2‑6份、潮州水洗泥8‑14份、北海白泥3‑6份和原矿黑泥2‑6份;所述脊性原料组与塑性原料组的原料重量份数比为0.7‑1:1。经过成分优化的本发明还提出了所述的高压注浆陶瓷浆料的制备方法,原料成分简单,可以有较好的过滤性,可以提升高压注浆时吸浆速度的速度。
High-pressure grouting ceramic slurry and preparation method thereof
一种高压注浆陶瓷浆料及其制备方法
HUANG TAO (author) / BAI JINGJING (author) / XUE FUQIN (author)
2020-11-03
Patent
Electronic Resource
Chinese
Double-liquid grouting slurry and preparation method thereof
European Patent Office | 2022
|Shield backfill grouting slurry and preparation method thereof
European Patent Office | 2024
|Shield backfill grouting slurry and preparation method thereof
European Patent Office | 2024
|Shield backfill grouting slurry and preparation method thereof
European Patent Office | 2021
|Shield grouting slurry, preparation method and construction device thereof
European Patent Office | 2020
|