A platform for research: civil engineering, architecture and urbanism
High-damping modified cement mortar and preparation method thereof
The invention relates to the technical field of building materials. The invention relates to high-damping modified cement mortar and a preparation method thereof. The high-damping modified cement mortar comprises components in parts by weight: 50-60 parts of cement, 100-120 parts of sand, 25-30 parts of water, 4-6 parts of styrene-acrylic emulsion, 0.2-0.5 part of water reducing agent, 0.1-0.3 part of defoaming agent, 1-3 parts of inner damping additive and 3-7 parts of outer damping additive. The inner damping additive is a stearic acid/butadiene rubber compound, and the outer damping additive is an erucyl amide/steel fiber/butadiene rubber compound. The high-damping modified cement mortar provided by the invention has the effect of improving the poor damping effect of the cement mortar.
本发明涉及建筑材料的技术领域,具体涉及一种高阻尼的改性水泥砂浆及其制备方法,其中,一种高阻尼的改性水泥砂浆,包括如下重量份数的组分:水泥50‑60份、砂100‑120份、水25‑30份、苯丙乳液4‑6份、减水剂0.2‑0.5份、消泡剂0.1‑0.3份、内阻尼添加料1‑3份、外阻尼添加料3‑7份,所述内阻尼添加料为硬脂酸/顺丁橡胶复配物,所述外阻尼添加料为芥酸酰胺/钢纤维/顺丁橡胶复配物。本发明提供的高阻尼的改性水泥砂浆具有改善水泥砂浆减震效果差的效果。
High-damping modified cement mortar and preparation method thereof
The invention relates to the technical field of building materials. The invention relates to high-damping modified cement mortar and a preparation method thereof. The high-damping modified cement mortar comprises components in parts by weight: 50-60 parts of cement, 100-120 parts of sand, 25-30 parts of water, 4-6 parts of styrene-acrylic emulsion, 0.2-0.5 part of water reducing agent, 0.1-0.3 part of defoaming agent, 1-3 parts of inner damping additive and 3-7 parts of outer damping additive. The inner damping additive is a stearic acid/butadiene rubber compound, and the outer damping additive is an erucyl amide/steel fiber/butadiene rubber compound. The high-damping modified cement mortar provided by the invention has the effect of improving the poor damping effect of the cement mortar.
本发明涉及建筑材料的技术领域,具体涉及一种高阻尼的改性水泥砂浆及其制备方法,其中,一种高阻尼的改性水泥砂浆,包括如下重量份数的组分:水泥50‑60份、砂100‑120份、水25‑30份、苯丙乳液4‑6份、减水剂0.2‑0.5份、消泡剂0.1‑0.3份、内阻尼添加料1‑3份、外阻尼添加料3‑7份,所述内阻尼添加料为硬脂酸/顺丁橡胶复配物,所述外阻尼添加料为芥酸酰胺/钢纤维/顺丁橡胶复配物。本发明提供的高阻尼的改性水泥砂浆具有改善水泥砂浆减震效果差的效果。
High-damping modified cement mortar and preparation method thereof
一种高阻尼的改性水泥砂浆及其制备方法
YANG XIAOHUA (author) / SU JUNHUI (author) / ZHOU CHENG (author) / CHEN QIANQIAN (author) / ZHONG LINYAN (author)
2020-11-20
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
High-damping modified cement mortar, preparation method and application thereof
European Patent Office | 2020
|High-damping modified cement mortar and preparation method and application thereof
European Patent Office | 2020
|Modified magnesium phosphate cement mortar and preparation method thereof
European Patent Office | 2021
|Nano-clay modified fiber cement mortar and preparation method thereof
European Patent Office | 2015
|Modified thermal insulation rubber cement mortar and preparation method thereof
European Patent Office | 2023
|