Dry-mixed mortar prepared from titanium extraction tailings
The invention belongs to the technical field of building materials, and particularly relates to dry-mixed mortar prepared from titanium extraction tailings. The invention provides the dry-mixed mortarprepared from titanium extraction tailings aims to overcome technical problems in the prior art. The dry-mixed mortar comprises the following components in parts by mass: 120-200 parts of cement, 90-160 parts of the titanium extraction tailings, 680-800 parts of sand and 2-3 parts of thickening powder. The industrial solid waste, namely the titanium extraction tailings are used in the dry-mixed mortar, the performance indexes such as the water retention rate, the strength grade, the softening coefficient and the maximum water absorption rate of the obtained dry-mixed mortar meet standard requirements, the strength grade and the water retention rate are superior to the strength grade and the water retention rate of common dry-mixed mortar, and the dry-mixed mortar can be widely applied toactual production.
本发明属于建筑材料技术领域,具体涉及提钛尾渣干混砂浆。本发明要解决的技术问题是提供一种以提钛尾渣为原料的干混砂浆,原料包括以下质量份的组分:水泥120~200份,提钛尾渣90~160份,砂680~800份,稠化粉2~3份。本发明将工业固体废弃物提钛尾渣在干混砂浆中进行了使用,所得干混砂浆的保水率、强度等级、软化系数、最大吸水率等性能指标满足规范要求,其中强度等级及保水率均优于普通干混砂浆,能够广泛应用于实际生产。
Dry-mixed mortar prepared from titanium extraction tailings
The invention belongs to the technical field of building materials, and particularly relates to dry-mixed mortar prepared from titanium extraction tailings. The invention provides the dry-mixed mortarprepared from titanium extraction tailings aims to overcome technical problems in the prior art. The dry-mixed mortar comprises the following components in parts by mass: 120-200 parts of cement, 90-160 parts of the titanium extraction tailings, 680-800 parts of sand and 2-3 parts of thickening powder. The industrial solid waste, namely the titanium extraction tailings are used in the dry-mixed mortar, the performance indexes such as the water retention rate, the strength grade, the softening coefficient and the maximum water absorption rate of the obtained dry-mixed mortar meet standard requirements, the strength grade and the water retention rate are superior to the strength grade and the water retention rate of common dry-mixed mortar, and the dry-mixed mortar can be widely applied toactual production.
本发明属于建筑材料技术领域,具体涉及提钛尾渣干混砂浆。本发明要解决的技术问题是提供一种以提钛尾渣为原料的干混砂浆,原料包括以下质量份的组分:水泥120~200份,提钛尾渣90~160份,砂680~800份,稠化粉2~3份。本发明将工业固体废弃物提钛尾渣在干混砂浆中进行了使用,所得干混砂浆的保水率、强度等级、软化系数、最大吸水率等性能指标满足规范要求,其中强度等级及保水率均优于普通干混砂浆,能够广泛应用于实际生产。
Dry-mixed mortar prepared from titanium extraction tailings
提钛尾渣干混砂浆
CHEN ZHIKE (author) / ZHAO YUJIE (author) / QIAN BAOJUN (author)
2020-12-01
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Cementing material prepared from titanium extraction tailings
European Patent Office | 2020
|European Patent Office | 2023
|Method for producing premixed dry-mixed mortar from iron tailings
European Patent Office | 2015
|Method for preparing superfine slag powder from titanium extraction tailings
European Patent Office | 2023
|