The invention relates to a symmetrical layered gradient composite material as well as a preparation method and application thereof, the method adopts a plasma activated sintering process to prepare amolybdenum/silicon nitride/molybdenum symmetrical layered gradient composite material, and the activation effect on powder particles before sintering is realized through the coupling effect of a temperature field, an electric field and a pressure field. Furthermore, the preparation of the gradient composite material is completed at a relatively low sintering temperature within a relatively short sintering time, and the molybdenum/silicon nitride/molybdenum symmetric layered gradient composite material with high density, low impurity content and good interface bonding is finally and quickly prepared by combining a plasma activated sintering method and the gradient of the gradient composite material.
本发明涉及一种对称层状梯度复合材料及其制备方法和应用,其中,所述方法采用等离子活化烧结工艺制备钼/氮化硅/钼对称层状梯度复合材料,通过温度场、电场以及压力场的耦合作用,实现了烧结前对粉体颗粒的活化作用,进而在较低烧结温度以及较短烧结时间内完成了梯度复合材料的制备,结合等离子活化烧结方法以及梯度复合材料的梯度化最终快速制得了致密度高、杂质含量少、界面结合好的钼/氮化硅/钼对称层状梯度复合材料。
Symmetrical layered gradient composite material and preparation method and application thereof
The invention relates to a symmetrical layered gradient composite material as well as a preparation method and application thereof, the method adopts a plasma activated sintering process to prepare amolybdenum/silicon nitride/molybdenum symmetrical layered gradient composite material, and the activation effect on powder particles before sintering is realized through the coupling effect of a temperature field, an electric field and a pressure field. Furthermore, the preparation of the gradient composite material is completed at a relatively low sintering temperature within a relatively short sintering time, and the molybdenum/silicon nitride/molybdenum symmetric layered gradient composite material with high density, low impurity content and good interface bonding is finally and quickly prepared by combining a plasma activated sintering method and the gradient of the gradient composite material.
本发明涉及一种对称层状梯度复合材料及其制备方法和应用,其中,所述方法采用等离子活化烧结工艺制备钼/氮化硅/钼对称层状梯度复合材料,通过温度场、电场以及压力场的耦合作用,实现了烧结前对粉体颗粒的活化作用,进而在较低烧结温度以及较短烧结时间内完成了梯度复合材料的制备,结合等离子活化烧结方法以及梯度复合材料的梯度化最终快速制得了致密度高、杂质含量少、界面结合好的钼/氮化硅/钼对称层状梯度复合材料。
Symmetrical layered gradient composite material and preparation method and application thereof
一种对称层状梯度复合材料及其制备方法和应用
CHEN FEI (author) / GU XING (author) / XU LI (author) / JIA MINGYONG (author) / WU YUEQI (author) / SHEN QIANG (author) / LI HUI (author) / XUE QING (author)
2020-12-08
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Layered gradient composite material as well as preparation method and application thereof
European Patent Office | 2022
|Gradient layered B4C-TiB2/Al composite material and preparation method thereof
European Patent Office | 2021
|European Patent Office | 2023
|European Patent Office | 2024
|Layered magnetoelectric composite material and preparation method thereof
European Patent Office | 2015
|