A platform for research: civil engineering, architecture and urbanism
The invention discloses a high-strength foamed cement block and a preparation method thereof. The high-strength foamed cement block comprises the following components, by mass: 2.2-3.0% of a reinforcing agent, 25-37% of an admixture, 0.05-0.10% of a vegetable protein foaming agent and 0.13-0.17% of HPMC (Hydroxy Propyl Methyl Cellulose) according to the mass ratio of P.O 42.5 ordinary Portland cement. According to the preparation method, a large amount of coal gangue, silica fume and chemical gypsum can be utilized, certain environmental protection benefits are achieved, the dry density of theprepared foamed cement block is 700 +/-30 kg/m <3>, the compressive strength is 8.0+/-0.3MPa and is higher than the strength of the foamed cement block under the same density, the performance of thefoamed cement block meets the requirements of FCB A 7.5 B 07 in JC/T 1062-2007, and a certain bearing effect is realized.
本发明公开了一种高强度发泡水泥砌块及其制备方法,按照P.O 42.5普通硅酸盐水泥质量比计如下:包括2.2‑3.0%增强剂、25‑37%掺合料、0.05‑0.10%植物蛋白发泡剂、0.13‑0.17%HPMC。该制备方法可大量利用煤矸石、硅灰以及化学石膏,具有一定的环保效益,其制备出的发泡水泥砌块干密度700±30kg/m3级,抗压强度8.0±0.3MPa,高于同级别密度下的发泡水泥砌块强度,其性能符合JC/T 1062‑2007中FCB A 7.5 B 07的要求,具有一定的承重效果。
The invention discloses a high-strength foamed cement block and a preparation method thereof. The high-strength foamed cement block comprises the following components, by mass: 2.2-3.0% of a reinforcing agent, 25-37% of an admixture, 0.05-0.10% of a vegetable protein foaming agent and 0.13-0.17% of HPMC (Hydroxy Propyl Methyl Cellulose) according to the mass ratio of P.O 42.5 ordinary Portland cement. According to the preparation method, a large amount of coal gangue, silica fume and chemical gypsum can be utilized, certain environmental protection benefits are achieved, the dry density of theprepared foamed cement block is 700 +/-30 kg/m <3>, the compressive strength is 8.0+/-0.3MPa and is higher than the strength of the foamed cement block under the same density, the performance of thefoamed cement block meets the requirements of FCB A 7.5 B 07 in JC/T 1062-2007, and a certain bearing effect is realized.
本发明公开了一种高强度发泡水泥砌块及其制备方法,按照P.O 42.5普通硅酸盐水泥质量比计如下:包括2.2‑3.0%增强剂、25‑37%掺合料、0.05‑0.10%植物蛋白发泡剂、0.13‑0.17%HPMC。该制备方法可大量利用煤矸石、硅灰以及化学石膏,具有一定的环保效益,其制备出的发泡水泥砌块干密度700±30kg/m3级,抗压强度8.0±0.3MPa,高于同级别密度下的发泡水泥砌块强度,其性能符合JC/T 1062‑2007中FCB A 7.5 B 07的要求,具有一定的承重效果。
High-strength foamed cement block and preparation method thereof
一种高强度发泡水泥砌块及其制备方法
2020-12-15
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Foamed ceramic and high-strength foamed cement composite board and preparation method thereof
European Patent Office | 2021
|High-strength fiber reinforced foamed cement insulation board and preparation method thereof
European Patent Office | 2020
|Light-weight and high-strength foamed magnesium oxysulfate cement and preparation method thereof
European Patent Office | 2020
|