Sleeve grouting material for steel bar connection and preparation method and application thereof
The invention provides a sleeve grouting material for steel bar connection and a preparation method and application thereof.The sleeve grouting material is composed of a component A and a component B.The component A is dry powder and comprises, by mass, 400-600 parts of cement, 10-40 parts of mineral admixture, 400-600 parts of sand, 0.2-3.0 parts of plastic expanding agent, 15-25 parts of expanding agent, 1-3 parts of water reducing agent, 0.2-1.0 part of defoaming agent, 0.1-1.0 part of stabilizer, 0-10 parts of antifreezing agent, 0-5 parts of an early strength agent, and 0-5 parts of a retarder; and the component B is water and comprises, in parts by mass, 120-170 parts of water. The sleeve grouting material has the characteristics of high fluidity, micro-expansion, high strength andthe like, and can be suitable for construction at different temperatures (-5 to 10 DEG C) and normal temperature (higher than 10 DEG C).
本发明提供一种钢筋连接用套筒灌浆料及其制备方法和应用,该灌浆料由A、B两组分组成,A组分为干粉料,按照质量份数计,包含水泥400~600份、矿物掺和料10~40份、砂400~600份、塑性膨胀剂0.2~3.0份、膨胀剂15~25份、减水剂1~3份、消泡剂0.2~1.0份、稳定剂0.1~1.0份、防冻剂0~10份、早强剂0~5份、缓凝剂0~5份;B组分为水,按照质量份数计,为120~170份。该灌浆料具有大流动性、微膨胀、高强度等特点,可以适用于低温(‑5~10℃)、常温(>10℃)不同温度施工。
Sleeve grouting material for steel bar connection and preparation method and application thereof
The invention provides a sleeve grouting material for steel bar connection and a preparation method and application thereof.The sleeve grouting material is composed of a component A and a component B.The component A is dry powder and comprises, by mass, 400-600 parts of cement, 10-40 parts of mineral admixture, 400-600 parts of sand, 0.2-3.0 parts of plastic expanding agent, 15-25 parts of expanding agent, 1-3 parts of water reducing agent, 0.2-1.0 part of defoaming agent, 0.1-1.0 part of stabilizer, 0-10 parts of antifreezing agent, 0-5 parts of an early strength agent, and 0-5 parts of a retarder; and the component B is water and comprises, in parts by mass, 120-170 parts of water. The sleeve grouting material has the characteristics of high fluidity, micro-expansion, high strength andthe like, and can be suitable for construction at different temperatures (-5 to 10 DEG C) and normal temperature (higher than 10 DEG C).
本发明提供一种钢筋连接用套筒灌浆料及其制备方法和应用,该灌浆料由A、B两组分组成,A组分为干粉料,按照质量份数计,包含水泥400~600份、矿物掺和料10~40份、砂400~600份、塑性膨胀剂0.2~3.0份、膨胀剂15~25份、减水剂1~3份、消泡剂0.2~1.0份、稳定剂0.1~1.0份、防冻剂0~10份、早强剂0~5份、缓凝剂0~5份;B组分为水,按照质量份数计,为120~170份。该灌浆料具有大流动性、微膨胀、高强度等特点,可以适用于低温(‑5~10℃)、常温(>10℃)不同温度施工。
Sleeve grouting material for steel bar connection and preparation method and application thereof
一种钢筋连接用套筒灌浆料及其制备方法和应用
JIA HENGQIONG (author) / WANG TAO (author) / ZHU HEQUAN (author) / DU CUNSHAN (author) / LI HAIYAN (author) / WEI ZHAO (author) / WU SHAOLIANG (author) / DU WEI (author) / YI ZHONGYU (author)
2021-01-05
Patent
Electronic Resource
Chinese
Grouting material for steel bar sleeve connection and preparation method and application thereof
European Patent Office | 2020
|Sleeve grouting material for steel bar connection and preparation method thereof
European Patent Office | 2020
|Sleeve grouting repairing material for steel bar connection and preparation method thereof
European Patent Office | 2023
|European Patent Office | 2022
|