Liquid alkali-free setting accelerator and preparation method thereof
The invention discloses a liquid alkali-free setting accelerator and a preparation method thereof. The liquid alkali-free setting accelerator is prepared from the following raw materials in percentageby weight: 40-70% of aluminum sulfate, 1-5% of a reinforcing agent, 0.1-5% of a dispersing agent, 0.1-1% of a thickening agent, 0.1-10% of organic alcohol amine and the balance of water, totaling 100%. The liquid alkali-free setting accelerator is prepared at normal temperature, extra heating is not needed in the production process, and energy conservation and environmental protection are achieved; wherein the mixing amount is 6-9%, the initial setting time is less than 5 minutes, the final setting time is less than 12 minutes, the one-day strength is more than 7 MPa, and the 28-day strengthis not lost; the storage stability is good, and precipitate and layering are avoided after 3 months.
本发明公开了一种液体无碱速凝剂及其制备方法,所述液体无碱速凝剂由如下重量百分比的原料组成:硫酸铝40‑70%,增强剂1‑5%,分散剂0.1‑5%,增稠剂0.1‑1%,有机醇胺0.1‑10%,余量为水,补足100%。所述的液体无碱速凝剂常温制备,生产过程无需额外加热,节能环保;掺量6‑9%,初凝时间小于5分钟,终凝时间小于12分钟,1天强度大于7兆帕,28天强度无损失;储存稳定性好,3个月无沉淀无分层。
Liquid alkali-free setting accelerator and preparation method thereof
The invention discloses a liquid alkali-free setting accelerator and a preparation method thereof. The liquid alkali-free setting accelerator is prepared from the following raw materials in percentageby weight: 40-70% of aluminum sulfate, 1-5% of a reinforcing agent, 0.1-5% of a dispersing agent, 0.1-1% of a thickening agent, 0.1-10% of organic alcohol amine and the balance of water, totaling 100%. The liquid alkali-free setting accelerator is prepared at normal temperature, extra heating is not needed in the production process, and energy conservation and environmental protection are achieved; wherein the mixing amount is 6-9%, the initial setting time is less than 5 minutes, the final setting time is less than 12 minutes, the one-day strength is more than 7 MPa, and the 28-day strengthis not lost; the storage stability is good, and precipitate and layering are avoided after 3 months.
本发明公开了一种液体无碱速凝剂及其制备方法,所述液体无碱速凝剂由如下重量百分比的原料组成:硫酸铝40‑70%,增强剂1‑5%,分散剂0.1‑5%,增稠剂0.1‑1%,有机醇胺0.1‑10%,余量为水,补足100%。所述的液体无碱速凝剂常温制备,生产过程无需额外加热,节能环保;掺量6‑9%,初凝时间小于5分钟,终凝时间小于12分钟,1天强度大于7兆帕,28天强度无损失;储存稳定性好,3个月无沉淀无分层。
Liquid alkali-free setting accelerator and preparation method thereof
一种液体无碱速凝剂及其制备方法
YAN XIAOWEI ( author ) / QIU XIRONG ( author ) / WANG ZHIMIN ( author ) / LIU QUANQING ( author ) / SU LEI ( author ) / FU TINGBO ( author ) / JIA WENLONG ( author ) / MA GAOFENG ( author ) / JIA JIPENG ( author )
2021-01-08
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Alkali-free liquid setting accelerator and preparation method thereof
European Patent Office | 2020
|European Patent Office | 2016
|Simple liquid alkali-free setting accelerator and preparation method thereof
European Patent Office | 2021
|Alkali-free liquid concrete setting accelerator and preparation method thereof
European Patent Office | 2015
|