Novel inorganic flame-retardant stone-like coating and preparation method thereof
The invention provides a novel inorganic flame-retardant stone-like coating. The novel inorganic flame-retardant stone-like coating is prepared by mixing and blending the following components in partsby weight: 80-120 parts of water, 1-3 parts of hydroxyethyl cellulose, 3-5 parts of an anionic dispersion stabilizer, 120-180 parts of potassium silicate, 50-100 parts of silica sol, 100-150 parts ofsilicon aerogel, 1-3 parts of a thickener and 510-613 parts of natural colored sand. The coating has the characteristics of flame retardancy, compactness, multicolor, scratch resistance, cracking resistance, dew formation resistance, mildew resistance, stain resistance, easiness in scrubbing, no smoke release, excellent storage stability and capability of being combined with a cement wall into awhole.
本发明提供一种新型无机阻燃真石漆,由如下重量份数的各组份混合调制得到:水80~120份、羟乙基纤维素1~3份、阴离子分散稳定剂3~5份、硅酸钾120~180份、硅溶胶50~100份、硅类气凝胶100~150份、增稠剂1~3份、天然彩砂510~613份。本发明具有阻燃、致密、多色、抗划伤,防开裂,防结露,防霉菌,耐沾污,易擦洗,无烟雾释放、储存稳定优、能与水泥墙体结合成一体的特点。
Novel inorganic flame-retardant stone-like coating and preparation method thereof
The invention provides a novel inorganic flame-retardant stone-like coating. The novel inorganic flame-retardant stone-like coating is prepared by mixing and blending the following components in partsby weight: 80-120 parts of water, 1-3 parts of hydroxyethyl cellulose, 3-5 parts of an anionic dispersion stabilizer, 120-180 parts of potassium silicate, 50-100 parts of silica sol, 100-150 parts ofsilicon aerogel, 1-3 parts of a thickener and 510-613 parts of natural colored sand. The coating has the characteristics of flame retardancy, compactness, multicolor, scratch resistance, cracking resistance, dew formation resistance, mildew resistance, stain resistance, easiness in scrubbing, no smoke release, excellent storage stability and capability of being combined with a cement wall into awhole.
本发明提供一种新型无机阻燃真石漆,由如下重量份数的各组份混合调制得到:水80~120份、羟乙基纤维素1~3份、阴离子分散稳定剂3~5份、硅酸钾120~180份、硅溶胶50~100份、硅类气凝胶100~150份、增稠剂1~3份、天然彩砂510~613份。本发明具有阻燃、致密、多色、抗划伤,防开裂,防结露,防霉菌,耐沾污,易擦洗,无烟雾释放、储存稳定优、能与水泥墙体结合成一体的特点。
Novel inorganic flame-retardant stone-like coating and preparation method thereof
一种新型无机阻燃真石漆及其制备方法
GU ERNING (author) / WANG PENGCHENG (author) / LIU SHUMIN (author) / HE WENMING (author) / FU CHAO (author)
2021-01-08
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Flame-retardant stone carton and preparation method thereof
European Patent Office | 2024
|Preparation method of inorganic external stone-like coating
European Patent Office | 2021
|European Patent Office | 2022
|Flame-retardant thermal-insulation coating and preparation method thereof
European Patent Office | 2020
|