A platform for research: civil engineering, architecture and urbanism
Gypsum self-leveling mortar capable of releasing negative oxygen ions
The invention relates to the technical field of self-leveling mortar, and discloses gypsum self-leveling mortar capable of releasing negative oxygen ions, which comprises the following components in percentage by weight: 20%-40% of ordinary portland cement, 10%-25% of high-alumina cement, 15%-30% of Portland cement, 10%-20% of an active master batch excitant, 25%-35% of synthetic resin, 10%-20% ofnoctilucent particles, 20%-30% of gypsum and 15%-25% of a mixed rare gem material. The preparation method comprises the following steps of: S1, respectively taking ordinary portland cement, high-alumina cement, Portland cement, an active master batch activator, synthetic resin, gypsum and a mixed rare gem material according to the weight percentages for later use; and S2, putting the ordinary portland cement, the high-alumina cement, the Portland cement, the active master batch excitant, the synthetic resin, the gypsum and the mixed rare gem material in the step S1 into a stirring device, andstirring at a speed of 200-300r/min until all the raw materials are uniformly mixed. The gypsum self-leveling mortar can release negative oxygen ions to purify the indoor air, the released negative oxygen ions can promote human health in the future use process, and the positive effects of environmental protection and home health are achieved.
本发明涉及自流平砂浆技术领域,且公开了一种释放负氧离子的石膏自流平砂浆,包括以下按重量百分比计的组分:普硅水泥20%‑40%,高铝水泥10%‑25%,硅酸盐水泥15%‑30%,活性母料激发剂10%‑20%,合成树脂25%‑35%,夜光颗粒10%‑20%,石膏20%‑30%,稀晶石15%‑25%,S1、按照以上重量百分比分别取普硅水泥、高铝水泥、硅酸盐水泥、活性母料激发剂、合成树脂、石膏和稀晶石备用;S2、将步骤S1中的普硅水泥、高铝水泥、硅酸盐水泥、活性母料激发剂、合成树脂、石膏和稀晶放入到搅拌装置中,以200‑300r/min的速度进行搅拌,直至各原料混合均匀;可以释放负氧离子,可以对室内的空气起到净化的作用,并且在日后的使用中,所释放的负氧离子可以促进人体健康,起到了环保且居家健康的积极作用。
Gypsum self-leveling mortar capable of releasing negative oxygen ions
The invention relates to the technical field of self-leveling mortar, and discloses gypsum self-leveling mortar capable of releasing negative oxygen ions, which comprises the following components in percentage by weight: 20%-40% of ordinary portland cement, 10%-25% of high-alumina cement, 15%-30% of Portland cement, 10%-20% of an active master batch excitant, 25%-35% of synthetic resin, 10%-20% ofnoctilucent particles, 20%-30% of gypsum and 15%-25% of a mixed rare gem material. The preparation method comprises the following steps of: S1, respectively taking ordinary portland cement, high-alumina cement, Portland cement, an active master batch activator, synthetic resin, gypsum and a mixed rare gem material according to the weight percentages for later use; and S2, putting the ordinary portland cement, the high-alumina cement, the Portland cement, the active master batch excitant, the synthetic resin, the gypsum and the mixed rare gem material in the step S1 into a stirring device, andstirring at a speed of 200-300r/min until all the raw materials are uniformly mixed. The gypsum self-leveling mortar can release negative oxygen ions to purify the indoor air, the released negative oxygen ions can promote human health in the future use process, and the positive effects of environmental protection and home health are achieved.
本发明涉及自流平砂浆技术领域,且公开了一种释放负氧离子的石膏自流平砂浆,包括以下按重量百分比计的组分:普硅水泥20%‑40%,高铝水泥10%‑25%,硅酸盐水泥15%‑30%,活性母料激发剂10%‑20%,合成树脂25%‑35%,夜光颗粒10%‑20%,石膏20%‑30%,稀晶石15%‑25%,S1、按照以上重量百分比分别取普硅水泥、高铝水泥、硅酸盐水泥、活性母料激发剂、合成树脂、石膏和稀晶石备用;S2、将步骤S1中的普硅水泥、高铝水泥、硅酸盐水泥、活性母料激发剂、合成树脂、石膏和稀晶放入到搅拌装置中,以200‑300r/min的速度进行搅拌,直至各原料混合均匀;可以释放负氧离子,可以对室内的空气起到净化的作用,并且在日后的使用中,所释放的负氧离子可以促进人体健康,起到了环保且居家健康的积极作用。
Gypsum self-leveling mortar capable of releasing negative oxygen ions
一种释放负氧离子的石膏自流平砂浆
YANG JINGLONG (author)
2021-03-16
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Gypsum plastering mortar capable of releasing negative oxygen ions
European Patent Office | 2021
|Gypsum self-leveling mortar capable of adsorbing formaldehyde
European Patent Office | 2021
|