Carbon-free steel ladle collector nozzle and preparation method thereof
The invention discloses a carbon-free steel ladle collector nozzle and a preparation method thereof, and belongs to the technical field of refractory materials, and the carbon-free steel ladle collector nozzle comprises the following components in percentage by weight: 60-64% of MAS-76 aluminum-magnesium spinel and 36-40% of co-grinding powder, totaling 100%; the co-grinding powder comprises 10%-18% of MAS-76 aluminum-magnesium spinel fine powder, 7%-13% of alpha-Al2O3 micro powder, 8%-10% of zirconite fine powder and 5% of metal silicon powder, and the thermosetting phenolic resin binding agent accounts for 4%-5% of the total weight of the co-grinding powder. According to the invention, MAS-76 aluminum-magnesium spinel is introduced as a granular aggregate, and through non-carbonization, the cleanliness quality of molten steel is improved, the product performance is improved, and the production cost is reduced; the carbon-free steel ladle collector nozzle has high temperature resistance, slag resistance and stripping resistance, and more MAS-76 aluminum-magnesium spinel particles and fine powder are distributed on the surface of the collector nozzle, so that the carbon-free steel ladle collector nozzle has good anti-scouring performance.
本发明公开了一种无碳钢包下水口及其制备方法,属于耐火材料技术领域,其组成成分及重量百分比为:MAS‑76铝镁尖晶石60%‑64%和共磨粉36%‑40%,总百分比为100%;外加占总重量百分比为4%~5%的热固酚醛树脂结合剂,其中共磨粉包括10%~18%MAS‑76铝镁尖晶石细粉、7%~13%α‑Al2O3微粉、8%~10%锆英石细粉和5%金属硅粉。本发明引入MAS‑76铝镁尖晶石作为颗粒骨料,通过无碳化,提高钢水洁净度质量,改善产品性能,降低生产成本;无碳钢包下水口具有耐高温性能、抗渣性能、抗剥落性能,且下水口表面分布有更多的MAS‑76铝镁尖晶石颗粒和细粉,具有很好的抗冲刷性能。
Carbon-free steel ladle collector nozzle and preparation method thereof
The invention discloses a carbon-free steel ladle collector nozzle and a preparation method thereof, and belongs to the technical field of refractory materials, and the carbon-free steel ladle collector nozzle comprises the following components in percentage by weight: 60-64% of MAS-76 aluminum-magnesium spinel and 36-40% of co-grinding powder, totaling 100%; the co-grinding powder comprises 10%-18% of MAS-76 aluminum-magnesium spinel fine powder, 7%-13% of alpha-Al2O3 micro powder, 8%-10% of zirconite fine powder and 5% of metal silicon powder, and the thermosetting phenolic resin binding agent accounts for 4%-5% of the total weight of the co-grinding powder. According to the invention, MAS-76 aluminum-magnesium spinel is introduced as a granular aggregate, and through non-carbonization, the cleanliness quality of molten steel is improved, the product performance is improved, and the production cost is reduced; the carbon-free steel ladle collector nozzle has high temperature resistance, slag resistance and stripping resistance, and more MAS-76 aluminum-magnesium spinel particles and fine powder are distributed on the surface of the collector nozzle, so that the carbon-free steel ladle collector nozzle has good anti-scouring performance.
本发明公开了一种无碳钢包下水口及其制备方法,属于耐火材料技术领域,其组成成分及重量百分比为:MAS‑76铝镁尖晶石60%‑64%和共磨粉36%‑40%,总百分比为100%;外加占总重量百分比为4%~5%的热固酚醛树脂结合剂,其中共磨粉包括10%~18%MAS‑76铝镁尖晶石细粉、7%~13%α‑Al2O3微粉、8%~10%锆英石细粉和5%金属硅粉。本发明引入MAS‑76铝镁尖晶石作为颗粒骨料,通过无碳化,提高钢水洁净度质量,改善产品性能,降低生产成本;无碳钢包下水口具有耐高温性能、抗渣性能、抗剥落性能,且下水口表面分布有更多的MAS‑76铝镁尖晶石颗粒和细粉,具有很好的抗冲刷性能。
Carbon-free steel ladle collector nozzle and preparation method thereof
一种无碳钢包下水口及其制备方法
FANG YANZHEN (author) / YU XIPING (author) / ZHAO FENG (author)
2021-05-07
Patent
Electronic Resource
Chinese
Steel ladle composite collector nozzle and preparation method thereof
European Patent Office | 2023
|European Patent Office | 2020
|European Patent Office | 2021
|Chromium-free fireclay for ladle sliding plate nozzle and preparation method thereof
European Patent Office | 2021
|Upper nozzle brick for steel ladle and preparation method of upper nozzle brick
European Patent Office | 2024
|