The invention discloses an environment-friendly brick and a production method thereof, and relates to the technical field of environment-friendly bricks. The environment-friendly brick is prepared from 30 to 50 parts of clay, 20 to 25 parts of shale, 12 to 24 parts of fly ash, 19 to 23 parts of corn straw, 12 to 16 parts of asphalt, 16 to 20 parts of ceramic fiber, 9 to 15 parts of river sand, 8 to 16 parts of bauxite, 7 to 13 parts of nano titanium dioxide, 5 to 10 parts of activated carbon and 8 to 12 parts of diatomite. According to the environment-friendly brick disclosed by the invention, by adding activated carbon and diatomite, the problem that the existing environment-friendly brick emits toxic and harmful gases such as formaldehyde and the like in an indoor decoration process is well solved, so that the harmful gases are better inhibited, and the harm of the harmful gases to human health is reduced; by adding nano titanium dioxide, the problem that a large amount of harmful gas is released in the firing process of the existing environment-friendly brick is well solved, the harmful gas in the firing process is reduced, and the environment is well protected; and through the fly ash and the straw, the problem of shortage of brick materials is well solved, and the purposes of energy conservation and environmental protection are achieved.
本发明公开了一种环保砖及其生产方法,涉及环保砖技术领域。本发明包括粘土30‑50份、页岩20‑25份、粉煤灰12‑24份、玉米秸秆19‑23份、沥青12‑16份、陶瓷纤维16‑20份、河砂9‑15份、铝矾土8‑16份、纳米二氧化钛7‑13份、活性炭5‑10份、硅藻土8‑12份。本发明通过通过添加活性炭和硅藻土很好的解决了现有的环保砖在室内装饰的过程中会散发出甲醛等有毒有害气体,使得对有害气体更好的抑制,降低有害气体对人体健康的危害,通过添加纳米二氧化钛使得很好的解决了现有环保砖烧制过程中会释放大量有害气体,使得降低了在烧制过程中的有害气体。使得对环境更好保护,通过粉煤灰和秸秆,很好地解决了砖材料紧缺的问题,达到了节能环保的目的。
The invention discloses an environment-friendly brick and a production method thereof, and relates to the technical field of environment-friendly bricks. The environment-friendly brick is prepared from 30 to 50 parts of clay, 20 to 25 parts of shale, 12 to 24 parts of fly ash, 19 to 23 parts of corn straw, 12 to 16 parts of asphalt, 16 to 20 parts of ceramic fiber, 9 to 15 parts of river sand, 8 to 16 parts of bauxite, 7 to 13 parts of nano titanium dioxide, 5 to 10 parts of activated carbon and 8 to 12 parts of diatomite. According to the environment-friendly brick disclosed by the invention, by adding activated carbon and diatomite, the problem that the existing environment-friendly brick emits toxic and harmful gases such as formaldehyde and the like in an indoor decoration process is well solved, so that the harmful gases are better inhibited, and the harm of the harmful gases to human health is reduced; by adding nano titanium dioxide, the problem that a large amount of harmful gas is released in the firing process of the existing environment-friendly brick is well solved, the harmful gas in the firing process is reduced, and the environment is well protected; and through the fly ash and the straw, the problem of shortage of brick materials is well solved, and the purposes of energy conservation and environmental protection are achieved.
本发明公开了一种环保砖及其生产方法,涉及环保砖技术领域。本发明包括粘土30‑50份、页岩20‑25份、粉煤灰12‑24份、玉米秸秆19‑23份、沥青12‑16份、陶瓷纤维16‑20份、河砂9‑15份、铝矾土8‑16份、纳米二氧化钛7‑13份、活性炭5‑10份、硅藻土8‑12份。本发明通过通过添加活性炭和硅藻土很好的解决了现有的环保砖在室内装饰的过程中会散发出甲醛等有毒有害气体,使得对有害气体更好的抑制,降低有害气体对人体健康的危害,通过添加纳米二氧化钛使得很好的解决了现有环保砖烧制过程中会释放大量有害气体,使得降低了在烧制过程中的有害气体。使得对环境更好保护,通过粉煤灰和秸秆,很好地解决了砖材料紧缺的问题,达到了节能环保的目的。
Environment-friendly ceramsite brick and production method thereof
European Patent Office | 2021
|Environment-friendly brick and preparation method thereof
European Patent Office | 2023
|Environment-friendly brick and preparation method thereof
European Patent Office | 2021
|Black sintered environment-friendly landscape brick and production method thereof
European Patent Office | 2015
|