A platform for research: civil engineering, architecture and urbanism
Ceramic lining composite steel pipe hole machining process
The invention discloses a ceramic lining composite steel pipe hole machining process. According to the technical scheme, the ceramic lining composite steel pipe hole machining process is characterized by comprising the following steps that S1, a seamless steel pipe is drilled through a drilling machine; s2, a transition object is selected, and the hole is plugged with the transition object; s3, the transition object is wrapped and fixed, ceramic mixed powder is added and sintering is performed; and S4, after sintering is completed, cooling is conducted, and then the transition object is taken out. The process adopted by the invention comprises the following steps: using the transition object, wrapping and fixing the transition object, adding ceramic mixed powder, sintering, cooling after sintering, and taking out the transition object to obtain the porous ceramic lining composite steel pipe with high precision and good aperture size; and the method is environment-friendly and can be recycled, the production cost is greatly reduced, and good economic benefits are obtained.
本发明公开了一种陶瓷内衬复合钢管孔加工工艺,其技术方案要点是:包括以下步骤:S1、先利用钻床在无缝钢管上钻孔;S2、选择过度物并用过度物塞住孔;S3、包裹固定过度物,加入陶瓷混合粉再进行烧结;S4、烧结完成后冷却再取出过度物。本发明采用的工艺为使用过度物,包裹固定过度物,加入陶瓷混合粉再进行烧结,烧结完成后冷却再取出过度物;就能得到精度高孔径尺寸良好的有孔陶瓷内衬复合钢管,这种方法环保并能循环利用,极大的降低了生产成本,取得了良好的经济效益。
Ceramic lining composite steel pipe hole machining process
The invention discloses a ceramic lining composite steel pipe hole machining process. According to the technical scheme, the ceramic lining composite steel pipe hole machining process is characterized by comprising the following steps that S1, a seamless steel pipe is drilled through a drilling machine; s2, a transition object is selected, and the hole is plugged with the transition object; s3, the transition object is wrapped and fixed, ceramic mixed powder is added and sintering is performed; and S4, after sintering is completed, cooling is conducted, and then the transition object is taken out. The process adopted by the invention comprises the following steps: using the transition object, wrapping and fixing the transition object, adding ceramic mixed powder, sintering, cooling after sintering, and taking out the transition object to obtain the porous ceramic lining composite steel pipe with high precision and good aperture size; and the method is environment-friendly and can be recycled, the production cost is greatly reduced, and good economic benefits are obtained.
本发明公开了一种陶瓷内衬复合钢管孔加工工艺,其技术方案要点是:包括以下步骤:S1、先利用钻床在无缝钢管上钻孔;S2、选择过度物并用过度物塞住孔;S3、包裹固定过度物,加入陶瓷混合粉再进行烧结;S4、烧结完成后冷却再取出过度物。本发明采用的工艺为使用过度物,包裹固定过度物,加入陶瓷混合粉再进行烧结,烧结完成后冷却再取出过度物;就能得到精度高孔径尺寸良好的有孔陶瓷内衬复合钢管,这种方法环保并能循环利用,极大的降低了生产成本,取得了良好的经济效益。
Ceramic lining composite steel pipe hole machining process
一种陶瓷内衬复合钢管孔加工工艺
ZHANG WENHONG (author)
2021-08-06
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Outer lining stainless steel composite steel pipe concrete member
European Patent Office | 2023
|Steel pipe based on Al2O3-SiO2-ZrO2 system ceramic lining and preparation method of steel pipe
European Patent Office | 2021
|Metal-ceramic composite steel pipe
British Library Online Contents | 1997
Epoxy Lining for Steel Water Pipe
Wiley | 1974
|Ceramic-Resin Lined Composite Steel Pipe
British Library Online Contents | 2000
|