The invention discloses non-stick heat-resistant ceramic pot glaze and a preparation method thereof, and relates to the technical field of preparation of ceramic pot glaze. The preparation method comprises the following steps: adding water into 2-4 parts of barium carbonate, 12-18 parts of calcined talc, 4-7 parts of sodium carbonate, 18-25 parts of glaze stone, 1-3 parts of tin oxide, 14-19 parts of silicon dioxide, 3-6 parts of zirconium dioxide, 2-5 parts of boron nitride, 7-16 parts of humite, 5-10 parts of diopside, 2-6 parts of nano silver-loaded zirconium silicate, 0.05-2 parts of nano zinc oxide, 10-40 parts of a quasicrystal material and 16-23 parts of fluororesin, mixing in a ball mill, and ball-milling for 5-12 hours to obtain the non-stick heat-resistant ceramic pot glaze. The quasicrystal material is added into the preparation raw materials of the ceramic glaze, the quasicrystal material is low in surface energy and good in adhesion resistance, and meanwhile, the quasicrystal material is high in hardness and low in friction coefficient, so that the quasicrystal material can greatly improve the hardness, wear resistance and corrosion resistance of the ceramic pot glaze, and even if a pot is sharp by an iron shovel, and the glaze of the ceramic pot cannot be damaged.
本发明公开了一种不粘耐热陶瓷锅釉及其制备方法,涉及陶瓷锅釉制备技术领域。本发明将碳酸钡2~4份,烧滑石12~18份,碳酸钠4~7份,釉果18~25份,氧化锡1~3份,二氧化硅14~19份,二氧化锆3~6份,氮化硼2~5份,硅镁石7~16份,透辉石5~10份,纳米硅酸锆载银2~6份,纳米氧化锌0.05~2份,准晶材料10‑40份,氟树脂16‑23份,加水混合到球磨机内,球磨5~12h,制得不粘耐热陶瓷锅釉,本发明通过在陶瓷釉的制备原料中加入准晶材料,准晶材料的表面能低,本身具有良好的抗粘性,同时准晶材料的硬度大、摩擦系数低,因此,准晶材料可以极大的提高陶瓷锅釉的硬度、耐磨性和耐腐蚀性能,即便使用铁铲尖锐锅具,也不会导致陶瓷锅釉被破坏。
The invention discloses non-stick heat-resistant ceramic pot glaze and a preparation method thereof, and relates to the technical field of preparation of ceramic pot glaze. The preparation method comprises the following steps: adding water into 2-4 parts of barium carbonate, 12-18 parts of calcined talc, 4-7 parts of sodium carbonate, 18-25 parts of glaze stone, 1-3 parts of tin oxide, 14-19 parts of silicon dioxide, 3-6 parts of zirconium dioxide, 2-5 parts of boron nitride, 7-16 parts of humite, 5-10 parts of diopside, 2-6 parts of nano silver-loaded zirconium silicate, 0.05-2 parts of nano zinc oxide, 10-40 parts of a quasicrystal material and 16-23 parts of fluororesin, mixing in a ball mill, and ball-milling for 5-12 hours to obtain the non-stick heat-resistant ceramic pot glaze. The quasicrystal material is added into the preparation raw materials of the ceramic glaze, the quasicrystal material is low in surface energy and good in adhesion resistance, and meanwhile, the quasicrystal material is high in hardness and low in friction coefficient, so that the quasicrystal material can greatly improve the hardness, wear resistance and corrosion resistance of the ceramic pot glaze, and even if a pot is sharp by an iron shovel, and the glaze of the ceramic pot cannot be damaged.
本发明公开了一种不粘耐热陶瓷锅釉及其制备方法,涉及陶瓷锅釉制备技术领域。本发明将碳酸钡2~4份,烧滑石12~18份,碳酸钠4~7份,釉果18~25份,氧化锡1~3份,二氧化硅14~19份,二氧化锆3~6份,氮化硼2~5份,硅镁石7~16份,透辉石5~10份,纳米硅酸锆载银2~6份,纳米氧化锌0.05~2份,准晶材料10‑40份,氟树脂16‑23份,加水混合到球磨机内,球磨5~12h,制得不粘耐热陶瓷锅釉,本发明通过在陶瓷釉的制备原料中加入准晶材料,准晶材料的表面能低,本身具有良好的抗粘性,同时准晶材料的硬度大、摩擦系数低,因此,准晶材料可以极大的提高陶瓷锅釉的硬度、耐磨性和耐腐蚀性能,即便使用铁铲尖锐锅具,也不会导致陶瓷锅釉被破坏。
Non-stick heat-resistant ceramic pot glaze and preparation method thereof
一种不粘耐热陶瓷锅釉及其制备方法
2021-09-17
Patent
Electronic Resource
Chinese
Corrosion-resistant ceramic glaze and preparation method thereof
European Patent Office | 2023
|Wear-resistant antibacterial ceramic glaze and preparation method thereof
European Patent Office | 2024
|High-hardness wear-resistant ceramic glaze and preparation method thereof
European Patent Office | 2020
|European Patent Office | 2020
|Wear-resistant dual-purpose ceramic glaze and preparation method thereof
European Patent Office | 2024
|