A platform for research: civil engineering, architecture and urbanism
Microcrystalline glaze, wear-resistant glaze, transparent microcrystalline wear-resistant full-polished glaze ceramic tile and preparation method
The invention relates to transparent microcrystalline glaze, a wear-resistant transparent glaze, a transparent microcrystalline wear-resistant full-polished glaze ceramic tile and a preparation method. The transparent microcrystalline glaze comprises the following components in parts by weight: 5 parts of barium carbonate; 18 parts of potassium feldspar; 9 parts of albite; 8 parts of aluminum oxide; 16 parts of calcite; 4 parts of quartz powder; 6 parts of dolomite; 10 parts of kaolin; 12 parts of calcined kaolin; 5 parts of wollastonite; 1 part of calcium fluoride; 1 part of titanium dioxide.The preparation method of the transparent microcrystalline wear-resistant full-polished glazed ceramic tile comprises the following steps: (1) pressing a green body; (2) applying/not applying groundcoat; (3) drying or not drying a glaze line; (4) carrying out comprehensive combined decoration including planographic printing, rubber roller printing, ink jet printing and the like; (5) drying or not drying a glaze line; (6) applying transparent microcrystalline glaze; (7) pouring/spraying wear-resistant transparent glaze; (8) performing firing in a kiln; and (9) conducting glaze polishing.
本发明涉及透明微晶釉、耐磨透明釉、透明微晶耐磨全抛釉瓷砖及制备方法,透明微晶釉按重量份:烧氧化锌5份;碳酸钡5份;钾长石18份;钠长石9份;氧化铝8份;方解石16份;石英粉4份;白云石6份;高岭土10份;煅烧高岭土12份;硅灰石5份;氟化钙1份;钛白粉1份。透明微晶耐磨全抛釉瓷砖的制备方法,包括:⑴坯体压制;⑵施/不施底釉;⑶釉线干燥或不干燥:⑷进行包括平板、胶辊、喷墨等综合组合装饰;⑸釉线干燥或不干燥;⑹施透明微晶釉;⑺淋/喷耐磨透明釉;⑻入窑烧成;⑼釉面抛光。
Microcrystalline glaze, wear-resistant glaze, transparent microcrystalline wear-resistant full-polished glaze ceramic tile and preparation method
The invention relates to transparent microcrystalline glaze, a wear-resistant transparent glaze, a transparent microcrystalline wear-resistant full-polished glaze ceramic tile and a preparation method. The transparent microcrystalline glaze comprises the following components in parts by weight: 5 parts of barium carbonate; 18 parts of potassium feldspar; 9 parts of albite; 8 parts of aluminum oxide; 16 parts of calcite; 4 parts of quartz powder; 6 parts of dolomite; 10 parts of kaolin; 12 parts of calcined kaolin; 5 parts of wollastonite; 1 part of calcium fluoride; 1 part of titanium dioxide.The preparation method of the transparent microcrystalline wear-resistant full-polished glazed ceramic tile comprises the following steps: (1) pressing a green body; (2) applying/not applying groundcoat; (3) drying or not drying a glaze line; (4) carrying out comprehensive combined decoration including planographic printing, rubber roller printing, ink jet printing and the like; (5) drying or not drying a glaze line; (6) applying transparent microcrystalline glaze; (7) pouring/spraying wear-resistant transparent glaze; (8) performing firing in a kiln; and (9) conducting glaze polishing.
本发明涉及透明微晶釉、耐磨透明釉、透明微晶耐磨全抛釉瓷砖及制备方法,透明微晶釉按重量份:烧氧化锌5份;碳酸钡5份;钾长石18份;钠长石9份;氧化铝8份;方解石16份;石英粉4份;白云石6份;高岭土10份;煅烧高岭土12份;硅灰石5份;氟化钙1份;钛白粉1份。透明微晶耐磨全抛釉瓷砖的制备方法,包括:⑴坯体压制;⑵施/不施底釉;⑶釉线干燥或不干燥:⑷进行包括平板、胶辊、喷墨等综合组合装饰;⑸釉线干燥或不干燥;⑹施透明微晶釉;⑺淋/喷耐磨透明釉;⑻入窑烧成;⑼釉面抛光。
Microcrystalline glaze, wear-resistant glaze, transparent microcrystalline wear-resistant full-polished glaze ceramic tile and preparation method
微晶釉、耐磨釉、透明微晶耐磨全抛釉瓷砖及制备方法
XIAO HUIYIN (author) / WANG YONGQIANG (author) / SHEN RONGWEI (author) / LIU RENSONG (author) / GU ZHANWEN (author) / CHEN ZHICHUAN (author) / LI ZHENJIN (author)
2020-08-18
Patent
Electronic Resource
Chinese
European Patent Office | 2024
|European Patent Office | 2022
|European Patent Office | 2024
|Microcrystalline transparent leadless glaze-polycrystalline micropowder-ceramic composite glass tile
European Patent Office | 2015
|