Corundum microporous aerator and production method thereof
The invention relates to a corundum microporous aerator and a production method thereof. The corundum microporous aerator comprises an upper corundum aeration body and a lower corundum aeration body, the upper corundum aeration body and the lower corundum aeration body are bonded and connected through adhesive glue, a mounting hole is formed in the center of the lower end of the lower corundum aeration body, the mounting hole is bonded with a connecting pipe through adhesive glue, each of the upper corundum body and the lower corundum body comprises 36# emery, 46# emery, 60# emery, kaolin, sawdust, flour, zinc oxide, barium oxide and water, all the components are reversely mixed and then enter a press to be pressed and formed, the adhesive glue comprises gelatin, gypsum, silica powder and zirconium oxide, and the upper corundum aeration body, the lower corundum aeration body and the connecting pipe are bonded through the adhesive glue and then fed into a kiln to be sintered and formed. The corundum microporous aerator is low in energy consumption, high in aeration efficiency, not prone to being broken or blocked and small in product resistance, and the service life is greatly prolonged.
本发明涉及一种刚玉微孔曝气器及其生产方法,包括上刚玉曝气体和下刚玉曝气体,所述上刚玉曝气体和下刚玉曝气体通过粘合胶粘合连接,所述下刚玉体下端中央开设安装孔,所述安装孔出通过粘合胶粘合连接管,所述上刚玉体和下刚玉体均包括36#刚玉砂、46#刚玉砂、60#刚玉砂、高岭土,木屑、面粉、氧化锌、氧化钡份和水,各组分逆向混料后进入压机内加压成型,所述粘合胶包括明胶、石膏、硅微粉和氧化锆,上刚玉曝气体、下刚玉曝气体和连接管通过粘合胶粘合好后送入窑炉烧结成型,所述刚玉微孔曝气器能耗低,曝气效率高,不易破碎,不易堵塞,产品阻力小,大大提高使用寿命。
Corundum microporous aerator and production method thereof
The invention relates to a corundum microporous aerator and a production method thereof. The corundum microporous aerator comprises an upper corundum aeration body and a lower corundum aeration body, the upper corundum aeration body and the lower corundum aeration body are bonded and connected through adhesive glue, a mounting hole is formed in the center of the lower end of the lower corundum aeration body, the mounting hole is bonded with a connecting pipe through adhesive glue, each of the upper corundum body and the lower corundum body comprises 36# emery, 46# emery, 60# emery, kaolin, sawdust, flour, zinc oxide, barium oxide and water, all the components are reversely mixed and then enter a press to be pressed and formed, the adhesive glue comprises gelatin, gypsum, silica powder and zirconium oxide, and the upper corundum aeration body, the lower corundum aeration body and the connecting pipe are bonded through the adhesive glue and then fed into a kiln to be sintered and formed. The corundum microporous aerator is low in energy consumption, high in aeration efficiency, not prone to being broken or blocked and small in product resistance, and the service life is greatly prolonged.
本发明涉及一种刚玉微孔曝气器及其生产方法,包括上刚玉曝气体和下刚玉曝气体,所述上刚玉曝气体和下刚玉曝气体通过粘合胶粘合连接,所述下刚玉体下端中央开设安装孔,所述安装孔出通过粘合胶粘合连接管,所述上刚玉体和下刚玉体均包括36#刚玉砂、46#刚玉砂、60#刚玉砂、高岭土,木屑、面粉、氧化锌、氧化钡份和水,各组分逆向混料后进入压机内加压成型,所述粘合胶包括明胶、石膏、硅微粉和氧化锆,上刚玉曝气体、下刚玉曝气体和连接管通过粘合胶粘合好后送入窑炉烧结成型,所述刚玉微孔曝气器能耗低,曝气效率高,不易破碎,不易堵塞,产品阻力小,大大提高使用寿命。
Corundum microporous aerator and production method thereof
一种刚玉微孔曝气器及其生产方法
QIAN GENGHUA (author) / WANG FENGJUN (author)
2021-10-22
Patent
Electronic Resource
Chinese
Microporous corundum castable and production method thereof
European Patent Office | 2022
|Microporous corundum brick and preparation method thereof
European Patent Office | 2023
|