Weather-resistant and aging-resistant cement-based flexible facing brick manufacturing method and manufactured flexible facing brick
A weather-resistant and aging-resistant cement-based flexible facing brick disclosed by the invention comprises a cement-based decorative layer and a cement-based matrix. The cement-based decorative layer is prepared from, by weight, 30-80 parts of cement, 30-80 parts of fine aggregate, 0.6-6 parts of pigment, 6-40 parts of mixed glue solution of polymer emulsion or redispersible polymer glue powder and water, and 3-20 parts of water. The cement-based matrix is prepared from, by weight, 30-80 parts of cement, 30-120 parts of fine aggregate, 6-40 parts of mixed glue solution of polymer emulsion or redispersible polymer glue powder and water, and 5-40 parts of water. The flexible facing brick has the remarkable advantages of extremely excellent durability and weather resistance. After 2160 hours of all-weather aging test, the performance of the flexible facing brick is still the same as that of cement mortar and even slightly improved, while the existing product can only lasts 500-1000 hours. The flexible facing brick is exquisite in decoration effect, excellent in comprehensive performance, low in cost and suitable for building outer walls, inner walls and roofs.
本发明所公开的一种耐候耐老化水泥基柔性饰面砖,包括水泥基装饰层和水泥基基体,所述水泥基装饰层包括重量份数的,水泥30~80份、细集料30~80份、颜料0.6~6份、聚合物乳液或可再分散聚合物胶粉与水的混合胶液6~40份、水3~20份;所述水泥基基体包括重量份数的:水泥30~80份、细集料30~120份、聚合物乳液或可再分散聚合物胶粉与水的混合胶液6~40份、水5~40份。显著优势:耐久、耐候性能极其优异。经全气候老化试验2160h,其性能仍然与水泥砂浆相同,甚至略有提高,而现有产品仅达到500~1000h。装饰效果精美,综合性能优,成本低,产品适用于建筑外墙、内墙、屋面。
Weather-resistant and aging-resistant cement-based flexible facing brick manufacturing method and manufactured flexible facing brick
A weather-resistant and aging-resistant cement-based flexible facing brick disclosed by the invention comprises a cement-based decorative layer and a cement-based matrix. The cement-based decorative layer is prepared from, by weight, 30-80 parts of cement, 30-80 parts of fine aggregate, 0.6-6 parts of pigment, 6-40 parts of mixed glue solution of polymer emulsion or redispersible polymer glue powder and water, and 3-20 parts of water. The cement-based matrix is prepared from, by weight, 30-80 parts of cement, 30-120 parts of fine aggregate, 6-40 parts of mixed glue solution of polymer emulsion or redispersible polymer glue powder and water, and 5-40 parts of water. The flexible facing brick has the remarkable advantages of extremely excellent durability and weather resistance. After 2160 hours of all-weather aging test, the performance of the flexible facing brick is still the same as that of cement mortar and even slightly improved, while the existing product can only lasts 500-1000 hours. The flexible facing brick is exquisite in decoration effect, excellent in comprehensive performance, low in cost and suitable for building outer walls, inner walls and roofs.
本发明所公开的一种耐候耐老化水泥基柔性饰面砖,包括水泥基装饰层和水泥基基体,所述水泥基装饰层包括重量份数的,水泥30~80份、细集料30~80份、颜料0.6~6份、聚合物乳液或可再分散聚合物胶粉与水的混合胶液6~40份、水3~20份;所述水泥基基体包括重量份数的:水泥30~80份、细集料30~120份、聚合物乳液或可再分散聚合物胶粉与水的混合胶液6~40份、水5~40份。显著优势:耐久、耐候性能极其优异。经全气候老化试验2160h,其性能仍然与水泥砂浆相同,甚至略有提高,而现有产品仅达到500~1000h。装饰效果精美,综合性能优,成本低,产品适用于建筑外墙、内墙、屋面。
Weather-resistant and aging-resistant cement-based flexible facing brick manufacturing method and manufactured flexible facing brick
一种耐候耐老化水泥基柔性饰面砖制作方法及所制作的柔性饰面砖
XU HU (author) / XU JINGXIU (author)
2021-11-09
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Corrosion-resistant weather-resistant mud brick and manufacturing method thereof
European Patent Office | 2020
|