The invention discloses a concrete filled steel tube and a preparation method thereof, relates to the technical field of concrete, and solves the technical problem of shrinkage cracking and even void of the concrete filled steel tube in the prior art. Per cubic meter of the concrete contains 550-580 kg of Portland cement, 40-45 kg of fly ash, 45-50 kg of silica fume, 950-980 kg of gravel, 700-720 kg of sand, 38-45 kg of a composite internal curing agent, 15-22 kg of a composite expanding agent, 5-6 kg of a polycarboxylic acid water reducing agent and 155-165 kg of water. The composite internal curing agent is a mixture of red water permeable brick particles and shale ceramsite, and the composite expanding agent is a mixture of magnesium oxide and calcium oxide. The concrete filled steel tube provided by the invention has the advantages of high anti-cracking grade and small shrinkage rate.
本发明公开了一种钢管混凝土及其制备方法,涉及混凝土技术领域,解决现有技术中钢管混凝土收缩开裂甚至脱空的技术问题,每立方米所述混凝土中含有以下质量的原材料:硅酸盐水泥550‑580kg,粉煤灰40‑45kg,硅灰45‑50kg,碎石950‑980kg,砂700‑720kg,复合内养护剂38‑45kg,复合膨胀剂15‑22kg,聚羧酸系减水剂5‑6kg,水155‑165kg,所述复合内养护剂为红色透水砖颗粒和页岩陶粒的混合物,所述复合膨胀剂为氧化镁和氧化钙的混合物;本发明所提供的钢管混凝土具有抗裂等级高、收缩率小的优点。
Concrete filled steel tube and preparation method thereof
The invention discloses a concrete filled steel tube and a preparation method thereof, relates to the technical field of concrete, and solves the technical problem of shrinkage cracking and even void of the concrete filled steel tube in the prior art. Per cubic meter of the concrete contains 550-580 kg of Portland cement, 40-45 kg of fly ash, 45-50 kg of silica fume, 950-980 kg of gravel, 700-720 kg of sand, 38-45 kg of a composite internal curing agent, 15-22 kg of a composite expanding agent, 5-6 kg of a polycarboxylic acid water reducing agent and 155-165 kg of water. The composite internal curing agent is a mixture of red water permeable brick particles and shale ceramsite, and the composite expanding agent is a mixture of magnesium oxide and calcium oxide. The concrete filled steel tube provided by the invention has the advantages of high anti-cracking grade and small shrinkage rate.
本发明公开了一种钢管混凝土及其制备方法,涉及混凝土技术领域,解决现有技术中钢管混凝土收缩开裂甚至脱空的技术问题,每立方米所述混凝土中含有以下质量的原材料:硅酸盐水泥550‑580kg,粉煤灰40‑45kg,硅灰45‑50kg,碎石950‑980kg,砂700‑720kg,复合内养护剂38‑45kg,复合膨胀剂15‑22kg,聚羧酸系减水剂5‑6kg,水155‑165kg,所述复合内养护剂为红色透水砖颗粒和页岩陶粒的混合物,所述复合膨胀剂为氧化镁和氧化钙的混合物;本发明所提供的钢管混凝土具有抗裂等级高、收缩率小的优点。
Concrete filled steel tube and preparation method thereof
一种钢管混凝土及其制备方法
ZHI CHENGYANG (author) / ZHI CHENGCHENG (author) / ZHI CHENGLIN (author) / ZHI GUANGXUN (author)
2021-12-21
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
C80 concrete, concrete filled steel tube and preparation method thereof
European Patent Office | 2020
|Phosphogypsum concrete-filled steel tube and preparation method thereof
European Patent Office | 2020
|Concrete-filled steel tube elastic sleeper and preparation method thereof
European Patent Office | 2023
|Prestressed concrete filled steel tube sleeper and preparation method thereof
European Patent Office | 2023
|