Environment-friendly construction method for asphalt road
The invention relates to an environment-friendly construction method for an asphalt road, and relates to the technical field of road engineering. The method comprises the four steps of paving the asphalt road, prefabricating a filling column, drilling a core for sampling and filling a sampling hole. The filling column is prefabricated by using an asphalt mixture, after the asphalt road is paved, the asphalt road is subjected to core drilling and sampling by using a drilling tool, and the drilling depth is limited during core drilling and sampling; after sampling is completed, the sampling hole is cleaned, and then the prefabricated filling plunger is plugged into the sampling hole to plug and fill up the sampling hole. The method has the advantages that the sampling hole filling effect is good, and the filling process is environmentally friendly.
本发明涉及一种沥青公路环保施工方法,涉及道路工程的技术领域,其包括沥青公路铺设,预制填补柱、钻芯取样和填补取样孔四个步骤,使用沥青混合料预制填补柱,在沥青公路铺设完成后,使用钻孔工具对沥青公路进行钻芯取样,并在钻芯取样时对钻孔的深度进行限定;在取样完成后,清理取样孔,然后将预制好的填补柱塞入取样孔中将取样孔封堵填平。本申请具有填补取样孔的效果好,填补过程绿色环保的效果。
Environment-friendly construction method for asphalt road
The invention relates to an environment-friendly construction method for an asphalt road, and relates to the technical field of road engineering. The method comprises the four steps of paving the asphalt road, prefabricating a filling column, drilling a core for sampling and filling a sampling hole. The filling column is prefabricated by using an asphalt mixture, after the asphalt road is paved, the asphalt road is subjected to core drilling and sampling by using a drilling tool, and the drilling depth is limited during core drilling and sampling; after sampling is completed, the sampling hole is cleaned, and then the prefabricated filling plunger is plugged into the sampling hole to plug and fill up the sampling hole. The method has the advantages that the sampling hole filling effect is good, and the filling process is environmentally friendly.
本发明涉及一种沥青公路环保施工方法,涉及道路工程的技术领域,其包括沥青公路铺设,预制填补柱、钻芯取样和填补取样孔四个步骤,使用沥青混合料预制填补柱,在沥青公路铺设完成后,使用钻孔工具对沥青公路进行钻芯取样,并在钻芯取样时对钻孔的深度进行限定;在取样完成后,清理取样孔,然后将预制好的填补柱塞入取样孔中将取样孔封堵填平。本申请具有填补取样孔的效果好,填补过程绿色环保的效果。
Environment-friendly construction method for asphalt road
一种沥青公路环保施工方法
ZHAN JIEHUA (author) / FENG DAOYAO (author) / CHEN FEIWEN (author)
2021-12-24
Patent
Electronic Resource
Chinese
IPC:
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
Novel environment-friendly modified asphalt road construction equipment and method
European Patent Office | 2023
|Environment-friendly asphalt structure and construction method thereof
European Patent Office | 2020
|Environment-friendly road construction device and construction method thereof
European Patent Office | 2024
|