Rock plate and preparation method thereof
The invention relates to a rock plate and a preparation method thereof. The preparation method comprises the following steps: preparing a green body; forming a cover glaze layer on the green body; forming a pattern layer on the cover glaze layer; sequentially applying stripping glaze containing a hydrophobic solvent and water-based glaze containing water on the pattern layer to form a grain layer; and forming a dry bead particle layer on the grain layer, wherein dry bead particles in the dry bead particle layer are spherical and are mainly prepared from the following raw materials in parts by weight: 30-45 parts of potassium feldspar, 6-10 parts of albite, 6-10 parts of kaolin, 10-20 parts of barium carbonate, 4-8 parts of wollastonite, 3-6 parts of zinc oxide, 4-8 parts of strontium carbonate, 7-13 parts of calcite, 1-4 parts of quartz and 1-5 parts of aluminum oxide. The rock plate prepared by the preparation method not only has better matte gloss, but also has concave-convex textures along lines on the surface; and the rock plate is combined with matte dry round bead particles for application, so high flatness, fine, smooth and mild hand feeling and good quality are achieved, and the application range of the rock plate can be widened.
本发明涉及一种岩板及其制备方法,包括以下步骤:制备坯体;在坯体上形成面釉层;在面釉层上形成图案层;在图案层上依次施加含疏水溶剂的剥开釉料和含水的水性釉料,形成纹路层;在纹路层上形成圆珠干粒层;圆珠干粒层中的圆珠干粒呈圆球状,且以重量份计,圆珠干粒主要由以下原料制备而成:钾长石30‑45份、钠长石6‑10份、高岭土6‑10份、碳酸钡10‑20份、硅灰石4‑8份、氧化锌3‑6份、碳酸锶4‑8份、方解石7‑13份、石英1‑4份及氧化铝1‑5份。该制备方法制备而成的岩板不仅具有较优的亚光光泽,且岩板表面具有沿着纹路的凹凸纹理,同亚光圆珠干粒结合应用,平整度较高,手感细腻温润,品质较优,能够扩宽其应用范围。
Rock plate and preparation method thereof
The invention relates to a rock plate and a preparation method thereof. The preparation method comprises the following steps: preparing a green body; forming a cover glaze layer on the green body; forming a pattern layer on the cover glaze layer; sequentially applying stripping glaze containing a hydrophobic solvent and water-based glaze containing water on the pattern layer to form a grain layer; and forming a dry bead particle layer on the grain layer, wherein dry bead particles in the dry bead particle layer are spherical and are mainly prepared from the following raw materials in parts by weight: 30-45 parts of potassium feldspar, 6-10 parts of albite, 6-10 parts of kaolin, 10-20 parts of barium carbonate, 4-8 parts of wollastonite, 3-6 parts of zinc oxide, 4-8 parts of strontium carbonate, 7-13 parts of calcite, 1-4 parts of quartz and 1-5 parts of aluminum oxide. The rock plate prepared by the preparation method not only has better matte gloss, but also has concave-convex textures along lines on the surface; and the rock plate is combined with matte dry round bead particles for application, so high flatness, fine, smooth and mild hand feeling and good quality are achieved, and the application range of the rock plate can be widened.
本发明涉及一种岩板及其制备方法,包括以下步骤:制备坯体;在坯体上形成面釉层;在面釉层上形成图案层;在图案层上依次施加含疏水溶剂的剥开釉料和含水的水性釉料,形成纹路层;在纹路层上形成圆珠干粒层;圆珠干粒层中的圆珠干粒呈圆球状,且以重量份计,圆珠干粒主要由以下原料制备而成:钾长石30‑45份、钠长石6‑10份、高岭土6‑10份、碳酸钡10‑20份、硅灰石4‑8份、氧化锌3‑6份、碳酸锶4‑8份、方解石7‑13份、石英1‑4份及氧化铝1‑5份。该制备方法制备而成的岩板不仅具有较优的亚光光泽,且岩板表面具有沿着纹路的凹凸纹理,同亚光圆珠干粒结合应用,平整度较高,手感细腻温润,品质较优,能够扩宽其应用范围。