A platform for research: civil engineering, architecture and urbanism
The invention discloses an early strength type regenerated slope protection brick which comprises cement, sulphoaluminate cement, regenerated machine-made sand dust collection powder, regenerated machine-made sand, regenerated concrete aggregate, regenerated decoration waste ground powder, an additive and water. The preparation method comprises the following steps: obtaining the admixture; weighing cement, sulphoaluminate cement, regenerated machine-made sand dust collection powder, regenerated machine-made sand, regenerated concrete aggregate and regenerated decoration waste ground powder in proportion to obtain first mixed powder ; putting the first mixed powder into a stirrer, and stirring for 5-10 seconds to obtain second mixed powder; adding the admixture and water into the second mixed powder, stirring for 60-120 seconds to obtain a mixture, and performing compression molding; and after molding, standing for 24-48 hours to obtain the early-strength regenerated slope protection brick. And by using the regenerated decoration garbage milled powder, the resource utilization of the decoration garbage is realized, the method is green and environment-friendly, the process is simple, and the method has important practical application value.
本发明公开了一种早强型再生护坡砖,包括:水泥、硫铝酸盐水泥、再生机制砂收尘粉、再生机制砂、再生砼骨料、再生装修垃圾磨粉料、外加剂、水。其制备方法,包括步骤:获得外加剂;按比例称取水泥、硫铝酸盐水泥、再生机制砂收尘粉、再生机制砂、再生砼骨料、再生装修垃圾磨粉料,获得第一混合粉料;将第一混合粉料置于搅拌机中,搅拌5‑10s,制得第二混合粉料;向第二混合粉料中加入所述外加剂与水,搅拌60‑120s,制得拌合物,压制成型;成型后静停24‑48h后,获得早强型再生护坡砖。使用再生装修垃圾磨粉料,实现了装修垃圾的资源化利用,绿色环保,工艺简单具有重要的实际应用价值。
The invention discloses an early strength type regenerated slope protection brick which comprises cement, sulphoaluminate cement, regenerated machine-made sand dust collection powder, regenerated machine-made sand, regenerated concrete aggregate, regenerated decoration waste ground powder, an additive and water. The preparation method comprises the following steps: obtaining the admixture; weighing cement, sulphoaluminate cement, regenerated machine-made sand dust collection powder, regenerated machine-made sand, regenerated concrete aggregate and regenerated decoration waste ground powder in proportion to obtain first mixed powder ; putting the first mixed powder into a stirrer, and stirring for 5-10 seconds to obtain second mixed powder; adding the admixture and water into the second mixed powder, stirring for 60-120 seconds to obtain a mixture, and performing compression molding; and after molding, standing for 24-48 hours to obtain the early-strength regenerated slope protection brick. And by using the regenerated decoration garbage milled powder, the resource utilization of the decoration garbage is realized, the method is green and environment-friendly, the process is simple, and the method has important practical application value.
本发明公开了一种早强型再生护坡砖,包括:水泥、硫铝酸盐水泥、再生机制砂收尘粉、再生机制砂、再生砼骨料、再生装修垃圾磨粉料、外加剂、水。其制备方法,包括步骤:获得外加剂;按比例称取水泥、硫铝酸盐水泥、再生机制砂收尘粉、再生机制砂、再生砼骨料、再生装修垃圾磨粉料,获得第一混合粉料;将第一混合粉料置于搅拌机中,搅拌5‑10s,制得第二混合粉料;向第二混合粉料中加入所述外加剂与水,搅拌60‑120s,制得拌合物,压制成型;成型后静停24‑48h后,获得早强型再生护坡砖。使用再生装修垃圾磨粉料,实现了装修垃圾的资源化利用,绿色环保,工艺简单具有重要的实际应用价值。
Early strength regenerated slope protection brick and preparation method thereof
一种早强型再生护坡砖及其制备方法
2022-01-21
Patent
Electronic Resource
Chinese
High-strength construction waste regenerated brick and preparation method thereof
European Patent Office | 2022
|Regenerated insulating brick and preparation method thereof
European Patent Office | 2022
|Regenerated landscape brick and preparation method thereof
European Patent Office | 2024
|Regenerated brick aggregate water permeable brick and preparation method thereof
European Patent Office | 2023
|Construction waste regenerated brick and preparation method thereof
European Patent Office | 2021
|