Regenerated brick aggregate water permeable brick and preparation method thereof
The invention discloses a recycled brick aggregate water permeable brick and a preparation method thereof. The recycled brick aggregate water permeable brick is prepared from the following components in parts by mass: 350 to 500 parts of cement, 10 to 100 parts of sulphoaluminate cement, 50 to 100 parts of red brick ground powder and 550 to 850 parts of No.1 brick aggregate, the recycled brick aggregate water permeable brick comprises, by weight, 100 parts of first brick aggregate, 200-500 parts of second brick aggregate, 500-900 parts of recycled machine-made sand, 10-50 parts of steel fibers, 8-20 parts of an additive and 180-240 parts of water, the particle size of the first brick aggregate is larger than or equal to 16 mm and smaller than or equal to 31.5 mm, the particle size of the second brick aggregate is larger than or equal to 5 mm and smaller than 16 mm, and the recycled brick aggregate water permeable brick is provided with a plurality of vertical channels penetrating in the thickness direction. A large amount of recycled brick aggregate is used as a main body material, resource utilization is achieved, meanwhile, strength, durability and water permeability are considered, and wide market prospects are achieved.
本发明公开了一种再生砖骨料透水砖及其制备方法,该再生砖骨料透水砖的质量份的组分为:水泥350‑500份、硫铝酸盐水泥10‑100份、红砖磨粉料50‑100份、一号砖骨料550‑850份;二号砖骨料200‑500份、再生机制砂500‑900份、钢纤维10‑50份、外加剂8‑20份、水180‑240份,其中,一号砖骨料的粒径大于等于16mm且小于等于31.5mm,二号砖骨料的粒径大于等于5mm且小于16mm,该再生砖骨料透水砖设有多个沿厚度方向贯穿的竖直通道。本发明主体材料使用了大量再生砖骨料,实现了资源化利用,同时兼顾了强度、耐久性和透水性,具有广阔的市场前景。
Regenerated brick aggregate water permeable brick and preparation method thereof
The invention discloses a recycled brick aggregate water permeable brick and a preparation method thereof. The recycled brick aggregate water permeable brick is prepared from the following components in parts by mass: 350 to 500 parts of cement, 10 to 100 parts of sulphoaluminate cement, 50 to 100 parts of red brick ground powder and 550 to 850 parts of No.1 brick aggregate, the recycled brick aggregate water permeable brick comprises, by weight, 100 parts of first brick aggregate, 200-500 parts of second brick aggregate, 500-900 parts of recycled machine-made sand, 10-50 parts of steel fibers, 8-20 parts of an additive and 180-240 parts of water, the particle size of the first brick aggregate is larger than or equal to 16 mm and smaller than or equal to 31.5 mm, the particle size of the second brick aggregate is larger than or equal to 5 mm and smaller than 16 mm, and the recycled brick aggregate water permeable brick is provided with a plurality of vertical channels penetrating in the thickness direction. A large amount of recycled brick aggregate is used as a main body material, resource utilization is achieved, meanwhile, strength, durability and water permeability are considered, and wide market prospects are achieved.
本发明公开了一种再生砖骨料透水砖及其制备方法,该再生砖骨料透水砖的质量份的组分为:水泥350‑500份、硫铝酸盐水泥10‑100份、红砖磨粉料50‑100份、一号砖骨料550‑850份;二号砖骨料200‑500份、再生机制砂500‑900份、钢纤维10‑50份、外加剂8‑20份、水180‑240份,其中,一号砖骨料的粒径大于等于16mm且小于等于31.5mm,二号砖骨料的粒径大于等于5mm且小于16mm,该再生砖骨料透水砖设有多个沿厚度方向贯穿的竖直通道。本发明主体材料使用了大量再生砖骨料,实现了资源化利用,同时兼顾了强度、耐久性和透水性,具有广阔的市场前景。
Regenerated brick aggregate water permeable brick and preparation method thereof
再生砖骨料透水砖及其制备方法
XIONG LEI (author) / SHANG LIJUAN (author) / JIN YANG (author) / ZHU LIULI (author) / YUE GANG (author)
2023-08-04
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Mixed fiber regenerated water permeable brick and preparation method thereof
European Patent Office | 2021
|European Patent Office | 2023
|European Patent Office | 2024
|Recycled aggregate water permeable brick and manufacturing method thereof
European Patent Office | 2020
|