The invention relates to an ecological-imitating stone and a preparation process thereof. The ecological-imitating stone is prepared from the following raw materials in parts by weight: 4 to 8 parts of crushed ore, 1 to 2 parts of slag powder, 0.5 to 1.5 parts of white cement and 0.1 to 0.3 part of cement modification enhancer. The ecological-imitating stone has a good technical standard, meets the technical requirements of A-class decoration materials in GB6566-2010 radionuclide limit of building materials through detection, meets the technical requirements of an appendix A of GB50209-2010 building ground engineering construction quality acceptance specification, meets the technical requirements of cement man-made in JC/T507-2012 terrazzo for building decoration, and the problems that natural marble is prone to fracture, low in strength, multiple in cracks, prone to alkali efflorescence and cracking after being laid and the like are solved, and the natural marble has the advantages of being anti-slip, wear-resistant, free of radiation, free of glue resin and the like.
本发明涉及一种仿生态石材及其制备工艺。所述仿生态石材包括如下重量份的原料:矿石碎料4~8份、矿渣粉1~2份、白水泥0.5~1.5份、水泥改性增强剂0.1~0.3份。所述仿生态石材具有良好的技术标准,经检测同时符合GB6566‑2010《建筑材料放射性核素限量》中A类装饰装修材料的技术要求,符合GB50209‑2010《建筑地面工程施工质量验收规范》附录A的技术要求,符合JC/T507‑2012《建筑装饰用水磨石》中水泥人造的技术要求,解决了天然大理石容易断裂、强度低、裂纹多、铺贴后易返碱、开裂等问题,并具有防滑、耐磨、无辐射、不含胶水树脂等优点。
The invention relates to an ecological-imitating stone and a preparation process thereof. The ecological-imitating stone is prepared from the following raw materials in parts by weight: 4 to 8 parts of crushed ore, 1 to 2 parts of slag powder, 0.5 to 1.5 parts of white cement and 0.1 to 0.3 part of cement modification enhancer. The ecological-imitating stone has a good technical standard, meets the technical requirements of A-class decoration materials in GB6566-2010 radionuclide limit of building materials through detection, meets the technical requirements of an appendix A of GB50209-2010 building ground engineering construction quality acceptance specification, meets the technical requirements of cement man-made in JC/T507-2012 terrazzo for building decoration, and the problems that natural marble is prone to fracture, low in strength, multiple in cracks, prone to alkali efflorescence and cracking after being laid and the like are solved, and the natural marble has the advantages of being anti-slip, wear-resistant, free of radiation, free of glue resin and the like.
本发明涉及一种仿生态石材及其制备工艺。所述仿生态石材包括如下重量份的原料:矿石碎料4~8份、矿渣粉1~2份、白水泥0.5~1.5份、水泥改性增强剂0.1~0.3份。所述仿生态石材具有良好的技术标准,经检测同时符合GB6566‑2010《建筑材料放射性核素限量》中A类装饰装修材料的技术要求,符合GB50209‑2010《建筑地面工程施工质量验收规范》附录A的技术要求,符合JC/T507‑2012《建筑装饰用水磨石》中水泥人造的技术要求,解决了天然大理石容易断裂、强度低、裂纹多、铺贴后易返碱、开裂等问题,并具有防滑、耐磨、无辐射、不含胶水树脂等优点。
Natural stone imitating ceramic tile and preparation process thereof
European Patent Office | 2022
|Inorganic artificial stone imitating natural marble texture and preparation process thereof
European Patent Office | 2022
|High-strength stone-imitating brick and preparation method thereof
European Patent Office | 2020
|Stone imitating water permeable brick and preparation method thereof
European Patent Office | 2020
|Artificial agglomerated stone imitating natural cracks and production process thereof
European Patent Office | 2021
|