The invention relates to the field of asphalt pavement maintenance, and particularly discloses a micro-surfacing mixture, a preparation method thereof and a micro-surfacing construction method. The micro-surfacing mixture is prepared from the following components in parts by weight: 100 to 132 parts of modified emulsified asphalt, 800 to 1200 parts of mineral aggregate, 90 to 100 parts of mixing water, 24 to 36 parts of oxidized polyethlene wax emulsion, 12 to 24 parts of silicon resin polyether emulsion and 8 to 18 parts of alloy powder. The micro-surfacing mixture disclosed by the invention can be used for repairing road ruts, and has the advantages of reducing the situation that the road ruts appear again and reducing the influence on the filling effect.
本申请涉及沥青路面养护的领域,具体公开了一种微表处混合料及其制备方法及微表处施工方法。一种微表处混合料包含以下重量份的组分:改性乳化沥青100~132份,矿料800~1200份,拌和用水90~100份,氧化聚乙烯蜡乳液24~36份,硅树脂聚醚乳液12~24份,合金粉末8~18份。本申请的微表处混合料可用于公路车辙修复,其具有减少公路再次出现车辙的情况,减少对填补效果的影响优点。
Micro-surfacing mixture, preparation method thereof and micro-surfacing construction method
The invention relates to the field of asphalt pavement maintenance, and particularly discloses a micro-surfacing mixture, a preparation method thereof and a micro-surfacing construction method. The micro-surfacing mixture is prepared from the following components in parts by weight: 100 to 132 parts of modified emulsified asphalt, 800 to 1200 parts of mineral aggregate, 90 to 100 parts of mixing water, 24 to 36 parts of oxidized polyethlene wax emulsion, 12 to 24 parts of silicon resin polyether emulsion and 8 to 18 parts of alloy powder. The micro-surfacing mixture disclosed by the invention can be used for repairing road ruts, and has the advantages of reducing the situation that the road ruts appear again and reducing the influence on the filling effect.
本申请涉及沥青路面养护的领域,具体公开了一种微表处混合料及其制备方法及微表处施工方法。一种微表处混合料包含以下重量份的组分:改性乳化沥青100~132份,矿料800~1200份,拌和用水90~100份,氧化聚乙烯蜡乳液24~36份,硅树脂聚醚乳液12~24份,合金粉末8~18份。本申请的微表处混合料可用于公路车辙修复,其具有减少公路再次出现车辙的情况,减少对填补效果的影响优点。
Micro-surfacing mixture, preparation method thereof and micro-surfacing construction method
一种微表处混合料及其制备方法及微表处施工方法
LIU YICHAO (author) / ZHANG CHI (author) / LI FENG (author) / ZHOU TAO (author) / YUAN XINGHUA (author) / LIU YUANHE (author) / ZHAN WANG (author) / WANG YANGFEI (author) / YUAN MAOXIANG (author)
2022-03-11
Patent
Electronic Resource
Chinese
Colored asphalt micro-surfacing mixture and preparation method thereof
European Patent Office | 2023
|MICRO-SURFACING SEALING COAT MIXTURE AND PREPARATION METHOD THEREOF
European Patent Office | 2022
|Micro-surfacing sealing coat mixture and preparation method thereof
European Patent Office | 2024
|Waste asphalt mixture regenerated micro-surfacing and preparation method thereof
European Patent Office | 2024
|