Environment-friendly building cement and preparation method thereof
The invention discloses environment-friendly building cement and a preparation method of the environment-friendly building cement. The invention relates to a cement brick, which comprises the following components in parts by weight: 40-60 parts of cement clinker, 6-9 parts of modified dried sludge, 5-10 parts of iron ore powder, 5-11 parts of desulfurized fly ash, 5-10 parts of limestone, 10-30 parts of sandstone, 10-20 parts of talcum powder, 10-20 parts of manganese slag and 15-30 parts of fluorgypsum. A preparation method of the cement brick comprises the following steps: S1, crushing treatment; s2, screening treatment work; s3, carrying out material body mixing treatment work; s4, uniformly dividing the material body; s5, sintering the clinker; according to the preparation method, efficient mixing of materials can be fully completed, the good mixing efficiency is achieved, the materials adhering to the inner wall of the mixing device can be effectively scraped off, waste of the materials is avoided, meanwhile, residues, waste materials and powder can be effectively and fully screened, and the powder can be fully mixed. And external uncrushed residues are discharged to the outside through the blanking disc.
本发明公开了一种环保建筑水泥及其制备方法,一种环保建筑水泥,包括按以下重量份原料制备得到;水泥熟料40‑60份、改性干化污泥6‑9份、铁矿粉5‑10份、脱硫灰5‑11份、石灰石5‑10份、砂岩10‑30份、滑石粉10‑20份、猛渣10‑20份、氟石膏15‑30份,其制备方法包括以下步骤:S1、破碎处理;S2、筛选处理工作;S3、料体混合处理工作;S4、料体均分处理工作;S5、熟料烧成工作;该制备方法不仅能够充分完成料体之间的高效混合,达到较好的混合效率,能够有效的将粘附于混合装置内壁上的料体进行刮除,从而避免料体造成浪费,同时也能够有效的将残渣废料以及粉体之间进行充分筛选,外部未粉碎的残渣通过下料盘向外部进行排出。
Environment-friendly building cement and preparation method thereof
The invention discloses environment-friendly building cement and a preparation method of the environment-friendly building cement. The invention relates to a cement brick, which comprises the following components in parts by weight: 40-60 parts of cement clinker, 6-9 parts of modified dried sludge, 5-10 parts of iron ore powder, 5-11 parts of desulfurized fly ash, 5-10 parts of limestone, 10-30 parts of sandstone, 10-20 parts of talcum powder, 10-20 parts of manganese slag and 15-30 parts of fluorgypsum. A preparation method of the cement brick comprises the following steps: S1, crushing treatment; s2, screening treatment work; s3, carrying out material body mixing treatment work; s4, uniformly dividing the material body; s5, sintering the clinker; according to the preparation method, efficient mixing of materials can be fully completed, the good mixing efficiency is achieved, the materials adhering to the inner wall of the mixing device can be effectively scraped off, waste of the materials is avoided, meanwhile, residues, waste materials and powder can be effectively and fully screened, and the powder can be fully mixed. And external uncrushed residues are discharged to the outside through the blanking disc.
本发明公开了一种环保建筑水泥及其制备方法,一种环保建筑水泥,包括按以下重量份原料制备得到;水泥熟料40‑60份、改性干化污泥6‑9份、铁矿粉5‑10份、脱硫灰5‑11份、石灰石5‑10份、砂岩10‑30份、滑石粉10‑20份、猛渣10‑20份、氟石膏15‑30份,其制备方法包括以下步骤:S1、破碎处理;S2、筛选处理工作;S3、料体混合处理工作;S4、料体均分处理工作;S5、熟料烧成工作;该制备方法不仅能够充分完成料体之间的高效混合,达到较好的混合效率,能够有效的将粘附于混合装置内壁上的料体进行刮除,从而避免料体造成浪费,同时也能够有效的将残渣废料以及粉体之间进行充分筛选,外部未粉碎的残渣通过下料盘向外部进行排出。
Environment-friendly building cement and preparation method thereof
一种环保建筑水泥及其制备方法
QI XIAOJIE (author) / YANG GUIRONG (author)
2022-04-12
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly cement and preparation method thereof
European Patent Office | 2021
|Environment-friendly cement and preparation method thereof
European Patent Office | 2021
|Environment-friendly Portland cement and preparation method thereof
European Patent Office | 2022
|Environment-friendly phosphogypsum cement and preparation method thereof
European Patent Office | 2023
|Environment-friendly Portland cement and preparation method thereof
European Patent Office | 2022
|