Coating material for iron ladle and torpedo ladle and preparation method of coating material
The invention discloses a coating material for iron ladles and torpedo ladles and a preparation method thereof, and the coating material comprises the following raw materials by weight: 10-30% of waste high alumina brick, 5-15% of waste silicon mold brick, 15-30% of waste dry quenching brick, 10-20% of waste iron runner material, 15-35% of aluminum-silicon dedusting ash, 0.5-3.0% of industrial desulfurization product MgSO4, and 8-15% of liquid binder. According to the present invention, the waste content in the used raw materials is high, the production cost is low, the production cost is reduced by about 75-90% compared with the traditional coating material, the use method of the coating material is simple, the coating material only needs to be manually coated to the to-be-repaired place, and the coating material has high refractoriness, and can adapt to the high temperature environment of 1300-1450 DEG C.
本发明公开了一种铁包与鱼雷罐用涂抹料及其制备方法,其中原料包括以下重量配比的成分,废高铝砖10~30%,废硅模砖5~15%,废干熄焦砖15~30%,废铁沟料10~20%,铝硅系除尘灰15~35%,工业脱硫产物MgSO4 0.5~3.0%,液体结合剂8~15%。本发明使用的原料中废弃物占比较高,生产成本较低,与传统涂抹料比生产成本降低约75%~90%,且该涂抹料在使用时方法简单,只需人工涂抹至需要修补的地方即可,且该涂抹料有较高的耐火度,能适应1300~1450℃的高温环境。
Coating material for iron ladle and torpedo ladle and preparation method of coating material
The invention discloses a coating material for iron ladles and torpedo ladles and a preparation method thereof, and the coating material comprises the following raw materials by weight: 10-30% of waste high alumina brick, 5-15% of waste silicon mold brick, 15-30% of waste dry quenching brick, 10-20% of waste iron runner material, 15-35% of aluminum-silicon dedusting ash, 0.5-3.0% of industrial desulfurization product MgSO4, and 8-15% of liquid binder. According to the present invention, the waste content in the used raw materials is high, the production cost is low, the production cost is reduced by about 75-90% compared with the traditional coating material, the use method of the coating material is simple, the coating material only needs to be manually coated to the to-be-repaired place, and the coating material has high refractoriness, and can adapt to the high temperature environment of 1300-1450 DEG C.
本发明公开了一种铁包与鱼雷罐用涂抹料及其制备方法,其中原料包括以下重量配比的成分,废高铝砖10~30%,废硅模砖5~15%,废干熄焦砖15~30%,废铁沟料10~20%,铝硅系除尘灰15~35%,工业脱硫产物MgSO4 0.5~3.0%,液体结合剂8~15%。本发明使用的原料中废弃物占比较高,生产成本较低,与传统涂抹料比生产成本降低约75%~90%,且该涂抹料在使用时方法简单,只需人工涂抹至需要修补的地方即可,且该涂抹料有较高的耐火度,能适应1300~1450℃的高温环境。
Coating material for iron ladle and torpedo ladle and preparation method of coating material
一种铁包与鱼雷罐用涂抹料及其制备方法
HE WENGUI (author) / ZHU LIFENG (author) / LI WEIDONG (author) / LI DALIN (author) / ZHANG MAO (author) / GUO PANLONG (author)
2022-05-27
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Heat insulation coating material for permanent layer of torpedo ladle
European Patent Office | 2021
|Improvement of shotcast material for torpedo ladle
Tema Archive | 2013
|Torpedo ladle lining smearing repair material, preparation method and use method
European Patent Office | 2020
|