A platform for research: civil engineering, architecture and urbanism
Building thermal insulation mortar with economic benefits
The invention provides a building thermal insulation mortar with economic benefits and a preparation method thereof. The building thermal insulation mortar with economic benefits is prepared from the following components in parts by weight: 200 to 600 parts of expanded perlite, 300 to 600 parts of cement, 50 to 150 parts of fly ash, 10 to 100 parts of heavy calcium powder, 0 to 50 parts of silica fume, 10 to 20 parts of redispersible latex powder, 1.0 to 4.0 parts of cellulose ether, 0 to 1.0 part of starch ether, 1 to 5 parts of polypropylene fiber, 0.01 to 1.5 parts of air entraining agent and 1000 to 1100 parts of water. The building thermal insulation mortar with economic benefits provided by the invention meets the II type performance index specified in the standard GB/T20473-2006 building thermal insulation mortar.
本发明提供一种具经济效益之建筑保温浆及其制备方法。所述具经济效益之建筑保温浆包括膨胀珍珠岩200‑600重量份,水泥300‑600重量份,粉煤灰50‑150重量份,重钙粉10‑100重量份,微硅粉0‑50重量份,可再分散乳胶粉10‑20重量份,纤维素醚1.0‑4.0重量份,淀粉醚0–1.0重量份,聚丙烯纤维1‑5重量份,引气剂0.01‑1.5重量份,水1000‑1100重量份。本发明提供所述具经济效益之建筑保温浆满足标准《GB/T20473‑2006建筑保温砂浆》中规定的II型性能指标。
Building thermal insulation mortar with economic benefits
The invention provides a building thermal insulation mortar with economic benefits and a preparation method thereof. The building thermal insulation mortar with economic benefits is prepared from the following components in parts by weight: 200 to 600 parts of expanded perlite, 300 to 600 parts of cement, 50 to 150 parts of fly ash, 10 to 100 parts of heavy calcium powder, 0 to 50 parts of silica fume, 10 to 20 parts of redispersible latex powder, 1.0 to 4.0 parts of cellulose ether, 0 to 1.0 part of starch ether, 1 to 5 parts of polypropylene fiber, 0.01 to 1.5 parts of air entraining agent and 1000 to 1100 parts of water. The building thermal insulation mortar with economic benefits provided by the invention meets the II type performance index specified in the standard GB/T20473-2006 building thermal insulation mortar.
本发明提供一种具经济效益之建筑保温浆及其制备方法。所述具经济效益之建筑保温浆包括膨胀珍珠岩200‑600重量份,水泥300‑600重量份,粉煤灰50‑150重量份,重钙粉10‑100重量份,微硅粉0‑50重量份,可再分散乳胶粉10‑20重量份,纤维素醚1.0‑4.0重量份,淀粉醚0–1.0重量份,聚丙烯纤维1‑5重量份,引气剂0.01‑1.5重量份,水1000‑1100重量份。本发明提供所述具经济效益之建筑保温浆满足标准《GB/T20473‑2006建筑保温砂浆》中规定的II型性能指标。
Building thermal insulation mortar with economic benefits
一种具经济效益之建筑保温浆
QIU XIUQIANG (author) / ZHU HONGGANG (author) / JIANG GUANG (author) / KUANG WENJIAN (author)
2022-06-03
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Building thermal insulation mortar formula and test method
European Patent Office | 2024
|European Patent Office | 2023
|Building thermal-insulation mortar and preparation method thereof
European Patent Office | 2015
|Novel thermal insulation mortar for building exterior walls
European Patent Office | 2020
|