The invention discloses energy-saving environment-friendly low-carbon leveling mortar and a preparation method thereof. The energy-saving environment-friendly low-carbon leveling mortar comprises the following components in percentage by weight: 20-40% of an active admixture, 1.0-25% of an alkaline material, 0.5-10% of an exciting agent, 30-80% of aggregate and 1.0-10% of a modified additive, the active admixture is prepared from superfine slag powder, superfine steel slag powder, fly ash, superfine lithium slag powder, superfine manganese slag powder and superfine phosphorus slag powder; the alkaline material is prepared from Portland cement, aluminate cement, sulphoaluminate cement, lime head, carbide slag and white mud; the exciting agent is prepared from ardealite, desulfurized gypsum, fluorgypsum, titanium gypsum, calcium chloride, calcium formate and sodium sulfate; the aggregate is prepared from copper tailing sand, iron tailing sand, manganese tailing sand, phosphorus tailing sand and quartz tailing sand. The production process is simple, the investment is small, the product performance is excellent, and the product belongs to an environment-friendly product and is wide in application scene.
本发明公开了一种节能环保型低碳找平砂浆及制备方法,包括以下重量配比组成:活性掺合料20~40%、碱性材料1.0~25%、激发剂0.5~10%、骨料30~80%、改性外加剂1.0~10%;所述活性掺合料由矿渣微粉、钢渣微粉、粉煤灰、锂渣微粉、锰渣微粉、磷渣微粉制成;所述碱性材料由硅酸盐水泥、铝酸盐水泥、硫铝酸盐水泥、石灰头、电石渣、白泥制成;所述激发剂由磷石膏、脱硫石膏、氟石膏、钛石膏、氯化钙、甲酸钙、硫酸钠制成;所述骨料由铜尾矿砂、铁尾矿砂、锰尾矿砂、磷尾矿砂、石英尾砂制成。本发明生产工艺简单,投资小,产品性能优异,属环境友好型产品,产品应用场景广阔。
Energy-saving environment-friendly low-carbon leveling mortar and preparation method thereof
The invention discloses energy-saving environment-friendly low-carbon leveling mortar and a preparation method thereof. The energy-saving environment-friendly low-carbon leveling mortar comprises the following components in percentage by weight: 20-40% of an active admixture, 1.0-25% of an alkaline material, 0.5-10% of an exciting agent, 30-80% of aggregate and 1.0-10% of a modified additive, the active admixture is prepared from superfine slag powder, superfine steel slag powder, fly ash, superfine lithium slag powder, superfine manganese slag powder and superfine phosphorus slag powder; the alkaline material is prepared from Portland cement, aluminate cement, sulphoaluminate cement, lime head, carbide slag and white mud; the exciting agent is prepared from ardealite, desulfurized gypsum, fluorgypsum, titanium gypsum, calcium chloride, calcium formate and sodium sulfate; the aggregate is prepared from copper tailing sand, iron tailing sand, manganese tailing sand, phosphorus tailing sand and quartz tailing sand. The production process is simple, the investment is small, the product performance is excellent, and the product belongs to an environment-friendly product and is wide in application scene.
本发明公开了一种节能环保型低碳找平砂浆及制备方法,包括以下重量配比组成:活性掺合料20~40%、碱性材料1.0~25%、激发剂0.5~10%、骨料30~80%、改性外加剂1.0~10%;所述活性掺合料由矿渣微粉、钢渣微粉、粉煤灰、锂渣微粉、锰渣微粉、磷渣微粉制成;所述碱性材料由硅酸盐水泥、铝酸盐水泥、硫铝酸盐水泥、石灰头、电石渣、白泥制成;所述激发剂由磷石膏、脱硫石膏、氟石膏、钛石膏、氯化钙、甲酸钙、硫酸钠制成;所述骨料由铜尾矿砂、铁尾矿砂、锰尾矿砂、磷尾矿砂、石英尾砂制成。本发明生产工艺简单,投资小,产品性能优异,属环境友好型产品,产品应用场景广阔。
Energy-saving environment-friendly low-carbon leveling mortar and preparation method thereof
一种节能环保型低碳找平砂浆及制备方法
JIN ZHOUBAO (author)
2023-03-28
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Energy-saving environment-friendly cement mortar and preparation method thereof
European Patent Office | 2020
|Energy-saving environment-friendly thermal-insulation mortar
European Patent Office | 2015
|European Patent Office | 2022
|